Dear Technos,
Does any of you have experience with wire bonding on quartz components?
Can ultrasonic bonding damage quartz or can it lift the Au plating from the quartz base material?
Any process related suggestions?
Thank you,
Ioan Tempea, P. Eng.
Senior Manufacturing Engineer, Satellite Systems
[cid:[log in to unmask]]
MacDonald, Dettwiler and Associates Corporation, 21025 Trans-Canada Highway, Ste-Anne-de-Bellevue, QC, Canada H9X 3R2
Tel: +1-514-457-2150 x3556
www.mdacorporation.com<http://www.mdacorporation.com/>
This e-mail, and any attachments, are intended solely for the use of the intended recipient(s) and may contain legally privileged, proprietary and/or confidential information. Any use, disclosure, dissemination, distribution or copying of this e-mail and any attachments for any purposes that have not been specifically authorized by the sender is strictly prohibited. If you are not the intended recipient, please immediately notify the sender by reply e-mail and permanently delete all copies and attachments. This email is for informational purposes only and shall not be interpreted to authorize or conclude a binding agreement between MDA and any other party unless this email contains or is accompanied by an express written confirmation of MDA's intention to enter into a binding agreement, such confirmation shall only be provided by an authorized representative of MDA.
|
|
|