adhesion not adhesive... correction...
On Aug 29, 2017, at 4:29 PM, Yuan-chia Joyce Koo wrote:
> aluminum wire bond? usually no problem on quartz, unless you
> directly bond on top of the structure (MEMS for example). As for
> gold plating lift off, either you have over travel of bond head
> (wedge), smash (force) too much, or your gold seed layer adhesive
> not strong enough (chemical seeding, instead of good
> sputtering)... IMHO (old info... more than 10 year old.. for your
> reference only).
> jk
> On Aug 29, 2017, at 1:49 PM, Ioan Tempea wrote:
>
>> Dear Technos,
>>
>> Does any of you have experience with wire bonding on quartz
>> components?
>>
>> Can ultrasonic bonding damage quartz or can it lift the Au plating
>> from the quartz base material?
>>
>> Any process related suggestions?
>>
>> Thank you,
>>
>> Ioan Tempea, P. Eng.
>> Senior Manufacturing Engineer, Satellite Systems
>>
>> [cid:[log in to unmask]]
>>
>> MacDonald, Dettwiler and Associates Corporation, 21025 Trans-
>> Canada Highway, Ste-Anne-de-Bellevue, QC, Canada H9X 3R2
>> Tel: +1-514-457-2150 x3556
>> www.mdacorporation.com<http://www.mdacorporation.com/>
>>
>> This e-mail, and any attachments, are intended solely for the use
>> of the intended recipient(s) and may contain legally privileged,
>> proprietary and/or confidential information. Any use, disclosure,
>> dissemination, distribution or copying of this e-mail and any
>> attachments for any purposes that have not been specifically
>> authorized by the sender is strictly prohibited. If you are not
>> the intended recipient, please immediately notify the sender by
>> reply e-mail and permanently delete all copies and attachments.
>> This email is for informational purposes only and shall not be
>> interpreted to authorize or conclude a binding agreement between
>> MDA and any other party unless this email contains or is
>> accompanied by an express written confirmation of MDA's intention
>> to enter into a binding agreement, such confirmation shall only be
>> provided by an authorized representative of MDA.
|