I seem to recall numerous industry articles (Pauls, Keeping, etc.) referencing that ideally the surface energy of a PCBA should be >~ 40 dyne cm prior to coating.
I have searched my files but cannot seem to find any of them now. Only some referencing the need to consider surface energy.
Does someone have any that reference " >~ 40 dyne cm prior to coating" readily available that they can forward to me?
Thanks
Rich Kraszewski
Senior Staff Process Engineer
Plexus Engineering Solutions
* * * * * * * * CONFIDENTIALITY NOTICE * * * * * * * *
This e-mail and any attachments are confidential from Plexus Corp. and may contain information which is privileged, confidential, and/or protected by non-disclosure agreements. They are intended solely for the use of the named addressee(s). . Any unauthorized use or disclosure may be unlawful. If you are not a named addressee, you must not use, disclose, retain or reproduce all or any part of the information contained in this e-mail or any attachments If you have received this transmission in error, please destroy it and notify us immediately by return e-mail or by calling + 1 888 208 9005.
|
|
|