TECHNET Archives

August 2017

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Show All Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Subject:
From:
"Decker, Scott UTAS" <[log in to unmask]>
Reply To:
TechNet E-Mail Forum <[log in to unmask]>, Decker, Scott UTAS
Date:
Fri, 18 Aug 2017 14:37:19 +0000
Content-Type:
text/plain
Parts/Attachments:
text/plain (1 lines)
Ah, what about “connection free”?  Seems that when “lead Free” doesn’t work, it becomes “Connection Free”…   Just saying….


Scott Decker – Staff Engineer, PCB Design Services CID+ – Electronic Systems Center
UTC AEROSPACE SYSTEMS
3445 S. 5th Street, Suite 170, Phoenix, AZ 85040 U.S.A.
Tel: 602 308 5957 FAX: 602 243 2347
[log in to unmask]<mailto:[log in to unmask]> www.utcaerospacesystems.com<http://www.utcaerospacesystems.com/>

CONFIDENTIALITY WARNING: This message may contain proprietary and/or privileged information of
UTC Aerospace Systems and its affiliated companies. If you are not the intended recipient please 1) do not disclose, copy,
distribute or use this message or its contents, 2) advise the sender by return e-mail, and 3) delete all copies (including all
attachments) from your computer. Your cooperation is greatly appreciated.
This Document Does Not Contain Export Controlled Technology Or Technical Data.

From: [log in to unmask] [mailto:[log in to unmask]]
Sent: Friday, August 18, 2017 7:31 AM
To: Decker, Scott UTAS; TechNet E-Mail Forum
Subject: Re: [TN] [External] Re: [TN] Soldering to 'Nickel-Silver'

Solder is the wrong terminology for anything lead free ........can we think of another term after 11 years??

Sent from my iPad Pro


On Fri, Aug 18, 2017 at 9:25 PM +0700, "Decker, Scott UTAS" <[log in to unmask]<mailto:[log in to unmask]>> wrote:

Wow! I didn't realize I was going to bring back so many memories of that wonderful "fragrance", Od-D-Rosin when I mentioned that, but seriously, I have almost a full roll of that multi core solder, (pronounced SOD DER) that I break out every so often to fix those devices that quit working. You know the ones they assemble with lead Free SOLD ER... :-) :-)

Happy Friday before the light goes out on Monday, Day! ;-)





Scott Decker – Staff Engineer, PCB Design Services CID+ – Electronic Systems Center

UTC AEROSPACE SYSTEMS

3445 S. 5th Street, Suite 170, Phoenix, AZ 85040 U.S.A.

Tel: 602 308 5957 FAX: 602 243 2347

[log in to unmask]<mailto:[log in to unmask]> www.utcaerospacesystems.com<http://www.utcaerospacesystems.com>



CONFIDENTIALITY WARNING: This message may contain proprietary and/or privileged information of

UTC Aerospace Systems and its affiliated companies. If you are not the intended recipient please 1) do not disclose, copy,

distribute or use this message or its contents, 2) advise the sender by return e-mail, and 3) delete all copies (including all

attachments) from your computer. Your cooperation is greatly appreciated.

This Document Does Not Contain Export Controlled Technology Or Technical Data.



-----Original Message-----

From: TechNet [mailto:[log in to unmask]] On Behalf Of John Burke

Sent: Friday, August 18, 2017 6:42 AM

To: [log in to unmask]<mailto:[log in to unmask]>

Subject: Re: [TN] [External] Re: [TN] Soldering to 'Nickel-Silver'











Yup it's been 48 years this year working in manufacturing...... and the smell of rosin cored solder is imprinted.....







Sent from my iPad Pro











On Fri, Aug 18, 2017 at 8:37 PM +0700, "Nutting, Phil" wrote:





















We are starting to show our age talking about wonderful smells from our formative years in electronics. Used some just the other day and the person looking over my shoulder commented on the nice smell, well I'd call it a fragrance.



-----Original Message-----

From: TechNet [mailto:[log in to unmask]] On Behalf Of John Burke

Sent: Friday, August 18, 2017 9:10 AM

To: [log in to unmask]<mailto:[log in to unmask]>

Subject: Re: [TN] [External] Re: [TN] Soldering to 'Nickel-Silver'













Ahhhhhh tin lead......... rosin cored solder.......lol





Sent from my iPad Pro













On Fri, Aug 18, 2017 at 3:59 AM +0700, "Decker, Scott UTAS" wrote:





















Many years ago, and I do mean many, my dad and grandfather had a large HO train layout and we used what was then called, (and may still be) nickel-Silver rail. This was back when we would get these 3 foot lengths of rail and spike it down to wooden roadbed. I think I was brass with a nickel plating, but I don't know for sure. What I do know is, it soldered really well with plane old rosin core lead solder. I can still remember the smell of those hot soldering guns... :-)



Scott Decker - Staff Engineer, PCB Design Services CID+ - Electronic Systems Center UTC AEROSPACE SYSTEMS

3445 S. 5th Street, Suite 170, Phoenix, AZ 85040 U.S.A.

Tel: 602 308 5957 FAX: 602 243 2347

[log in to unmask]<mailto:[log in to unmask]> www.utcaerospacesystems.com<http://www.utcaerospacesystems.com>



CONFIDENTIALITY WARNING: This message may contain proprietary and/or privileged information of UTC Aerospace Systems and its affiliated companies. If you are not the intended recipient please 1) do not disclose, copy, distribute or use this message or its contents, 2) advise the sender by return e-mail, and 3) delete all copies (including all

attachments) from your computer. Your cooperation is greatly appreciated.

This Document Does Not Contain Export Controlled Technology Or Technical Data.



-----Original Message-----

From: TechNet [mailto:[log in to unmask]] On Behalf Of George Wenger

Sent: Thursday, August 17, 2017 1:53 PM

To: [log in to unmask]<mailto:[log in to unmask]>

Subject: [External] Re: [TN] Soldering to 'Nickel-Silver'



Yea since it is a copper alloy German-Silver and Nickel-Silver do seem like crazy names since there is no silver in the alloy but a lot of times things get named for what they look like and when you look at something made from this alloy it has a nickel or silver color and not a copper color.





-----Original Message-----

From: TechNet [mailto:[log in to unmask]] On Behalf Of Giamis, Andy

Sent: Thursday, August 17, 2017 4:47 PM

To: [log in to unmask]<mailto:[log in to unmask]>

Subject: Re: [TN] Soldering to 'Nickel-Silver'



Thanks George,

I'll play around a little and see what sticks.

Gotta love these crazy alloy names: German-Silver, Nickel-Silver, etc. And not a lick of silver in it.





-----Original Message-----

From: TechNet [mailto:[log in to unmask]] On Behalf Of George Wenger

Sent: Thursday, August 17, 2017 3:38 PM

To: [log in to unmask]<mailto:[log in to unmask]>

Subject: Re: [TN] Soldering to 'Nickel-Silver'



Andy,



I somewhat agree with Bev that some of the no-clean solder pastes and fluxes should allow you to solder to Nickel-Silver. I disagree that is commonly referred to as German Silver. Since he's from Canada it may commonly be referred to there and in Europe as German Silver but in my 40 years in telecommunication equipment soldering I've commonly heard it referred to as Nickel-Silver.



I also agree with Phil, any flux that contains zinc chloride and HCl should solder almost any metal.



You might also want to try soldering with a standard WSF and you should have success.



My other recommendation is to do solderability testing in your analysis lab and she what flux works



George



-----Original Message-----

From: TechNet [mailto:[log in to unmask]] On Behalf Of Bev Christian

Sent: Thursday, August 17, 2017 4:12 PM

To: [log in to unmask]<mailto:[log in to unmask]>

Subject: Re: [TN] Soldering to 'Nickel-Silver'



Andy,

This is commonly referred to as German Silver. I have seen it often used for RF cans. It should solder fine with your usual non-clean solder pastes.

However, will the can warp? We set specific maximum sizes for different shapes of RF cans (not that the designers would always listen). We also measured can warpage using shadow moiré.



Regards,

Bev Christian

HDP User Group



-----Original Message-----

From: TechNet [mailto:[log in to unmask]] On Behalf Of Giamis, Andy

Sent: Thursday, August 17, 2017 3:38 PM

To: [log in to unmask]<mailto:[log in to unmask]>

Subject: [TN] Soldering to 'Nickel-Silver'



Hi Folks,

Has anyone had experience soldering to 'Nickel-Silver'

This is a ternary alloy with approximately 60% Cu, 20% Ni, 20% Zn.



If so, are there any special considerations such as flux type, pre-tinning etc...







Best Regards,

Andy

Senior Failure Analysis Engineer