TECHNET Archives

August 2017

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Show All Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Subject:
From:
George Wenger <[log in to unmask]>
Reply To:
TechNet E-Mail Forum <[log in to unmask]>, George Wenger <[log in to unmask]>
Date:
Thu, 17 Aug 2017 16:52:43 -0400
Content-Type:
text/plain
Parts/Attachments:
text/plain (83 lines)
Yea since it is a copper alloy German-Silver and Nickel-Silver do seem like
crazy names since there is no silver in the alloy but a lot of times things
get named for what they look like and when you look at something made from
this alloy it has a nickel or silver color and not a copper color.


-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Giamis, Andy
Sent: Thursday, August 17, 2017 4:47 PM
To: [log in to unmask]
Subject: Re: [TN] Soldering to 'Nickel-Silver'

Thanks George,
I'll play around a little and see what sticks.
Gotta love these crazy alloy names: German-Silver, Nickel-Silver, etc. And
not a lick of silver in it.


-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of George Wenger
Sent: Thursday, August 17, 2017 3:38 PM
To: [log in to unmask]
Subject: Re: [TN] Soldering to 'Nickel-Silver'

Andy,

I somewhat agree with Bev that some of the no-clean solder pastes and fluxes
should allow you to solder to Nickel-Silver. I disagree that is commonly
referred to as German Silver. Since he's from Canada it may commonly be
referred to there and in Europe as German Silver but in my 40 years in
telecommunication equipment soldering I've commonly heard it referred to as
Nickel-Silver.

I also agree with Phil, any flux that contains zinc chloride and HCl should
solder almost any metal.

You might also want to try soldering with a standard WSF and you should have
success.

My other recommendation is to do solderability testing in your analysis lab
and she what flux works

George

-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Bev Christian
Sent: Thursday, August 17, 2017 4:12 PM
To: [log in to unmask]
Subject: Re: [TN] Soldering to 'Nickel-Silver'

Andy,
This is commonly referred to as German Silver. I have seen it often used
for RF cans. It should solder fine with your usual non-clean solder pastes.
However, will the can warp? We set specific maximum sizes for different
shapes of RF cans (not that the designers would always listen). We also
measured can warpage using shadow moiré.

Regards,
Bev Christian
HDP User Group

-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Giamis, Andy
Sent: Thursday, August 17, 2017 3:38 PM
To: [log in to unmask]
Subject: [TN] Soldering to 'Nickel-Silver'

Hi Folks,
Has anyone had experience soldering to 'Nickel-Silver'
This is a ternary alloy with approximately 60% Cu, 20% Ni, 20% Zn.

If so, are there any special considerations such as flux type, pre-tinning
etc...



Best Regards,
Andy
Senior Failure Analysis Engineer
CommScope
2601 Telecom Pkwy
Richardson, TX, 75082, USA