TECHNET Archives

August 2017

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Show All Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Subject:
From:
David Hillman <[log in to unmask]>
Reply To:
TechNet E-Mail Forum <[log in to unmask]>, David Hillman <[log in to unmask]>
Date:
Tue, 29 Aug 2017 07:52:21 -0500
Content-Type:
text/plain
Parts/Attachments:
text/plain (96 lines)
Hi guys - yep, I know exactly what inductor component we are discussing.
The flattened copper wire isn't the problem - we chased through that on a
similar issue to what Steve describes and found it really wasn't playing a
role. The simple answer is that Ag/Pd/Pt termination finishes don't have
good long term solderability, have a very narrow soldering process window
because they would rather dissolve into the solder joint than stay on the
component termination and can have inconsistent wetting forces which causes
them to shift around on their pads - all of the things that Steve
described! The only suggestions I can offer than help reduce the problems
are to make sure your reflow profile is fully characterized, look at your
pad geometries to make sure they are not oversized and more active fluxes
can help with the wetting.

Dave Hillman
Rockwell Collins
[log in to unmask]

On Mon, Aug 28, 2017 at 10:32 AM, Bev Christian <[log in to unmask]>
wrote:

> Steve,
> I forgot to ask, what type of flux are you using? I remember discussing in
> the IPC J-002 committee that some no-clean fluxes are better than others
> for soldering application with a palladium finish. I wonder if that is in
> play here? I expect Dave Hillman to have more to say about this.
> Bev
>
> -----Original Message-----
> From: TechNet [mailto:[log in to unmask]] On Behalf Of Vargas, Stephen M
> Sent: Monday, August 28, 2017 11:25 AM
> To: [log in to unmask]
> Subject: Re: [TN] EXTERNAL: RE: [TN] Odd Finish Soldering
>
> Bev:
>
> Yes, the end of the copper winding is embedded in the bottom
> termination and does not appear to be covered by the finish. It actually
> looks like the copper wire has been compressed to produce a more flattened
> surface. I suspect oxidation of this wire is contributing to our problem,
> but I've also read (back from 2008) that this finish will dissolve into
> solder causing non-optimized soldering angles which can cause premature
> failure during shock and vibe testing. I'm trying to determine if this
> theory still holds true today. Thanks again.
>
> Regards,
> Steve Vargas
>
> If you don't have time to do it right, when will you have time to do it
> over?
> John Wooden
>
> Polaris Contract Mfg Inc
> 15 Barnabas Rd
> Marion, MA 02738
> 774-553-6192
> [log in to unmask]
>
>  Please consider the environment before printing this e-mail
>
> -----Original Message-----
> From: Bev Christian [mailto:[log in to unmask]]
> Sent: Monday, August 28, 2017 11:04 AM
> To: 'TechNet E-Mail Forum' <[log in to unmask]>; Vargas, Stephen M (US) <
> [log in to unmask]>
> Subject: EXTERNAL: RE: [TN] Odd Finish Soldering
>
> Steve,
> Is the problem the finish or does the inductor have the end of the copper
> winding embedded in the bottom termination finish but it is not totally
> covered by that finish? If so, then the oxidized copper wiring is your
> problem, not the termination finish. I have run into this before. Why the
> manufacturers insist on terminating the wire on the bottom rather than the
> top is beyond me.
>
> Bev
>
> -----Original Message-----
> From: TechNet [mailto:[log in to unmask]] On Behalf Of Vargas, Stephen M
> Sent: Monday, August 28, 2017 10:38 AM
> To: [log in to unmask]
> Subject: [TN] Odd Finish Soldering
>
> Good morning:
>
> We've experienced some soldering difficulties with small 0402
> inductors using a silver palladium platinum glass plating. Our application
> is a 63/37 process and we find that these parts shift randomly through our
> reflow oven and the overall soldering is less than optimum. The part is
> available in a more robust plating, but the cost impact is absurd. I'm
> wondering if others have run into similar problems with this finish and why
> the difficulty in soldering these parts. Thanks in advance.
>
> Regards,
> Steve Vargas
>

ATOM RSS1 RSS2