Hi Rich - I have a number of good references sources and do track this as a
topic and that is the first time I have heard that silicon was an issue. I
suspect they may be confusing fracking sand versus other sand
type/applications as that is a hot topic. I would love to see their
reference data as it sounds quite suspicious.
Dave Hillman
Rockwell Collins
[log in to unmask]
On Tue, Jul 25, 2017 at 1:12 PM, Richard Kraszewski <
[log in to unmask]> wrote:
> Last week I heard an interesting story NPR radio, claiming that there
> is an upcoming global scarcity of sand.
>
> Seems like most good deposits are being mined out for concrete. This is
> starting to become a concern for people such as silicon wafer producers
> amongst others.
>
>
>
> Anyone hear anything similar?
>
>
> Rich Kraszewski
> Senior Staff Process Engineer
> Plexus Engineering Solutions
>
>
> * * * * * * * * CONFIDENTIALITY NOTICE * * * * * * * *
>
> This e-mail and any attachments are confidential from Plexus Corp. and may
> contain information which is privileged, confidential, and/or protected by
> non-disclosure agreements. They are intended solely for the use of the
> named addressee(s). . Any unauthorized use or disclosure may be
> unlawful. If you are not a named addressee, you must not use, disclose,
> retain or reproduce all or any part of the information contained in this
> e-mail or any attachments If you have received this transmission in error,
> please destroy it and notify us immediately by return e-mail or by calling +