Subject: | |
From: | |
Reply To: | |
Date: | Wed, 14 Jun 2017 15:46:34 -0500 |
Content-Type: | text/plain |
Parts/Attachments: |
|
|
Hi Rich - don't know if its helpful but even XY is permeable to vapors -
its just a couple of orders of magnitude better than the other typical
conformal coatings.
Dave
On Wed, Jun 14, 2017 at 1:43 PM, Richard Kraszewski <
[log in to unmask]> wrote:
> Does anyone know if a special coating type would be
> required/recommended for a medical Ethylene Oxide sterilization process?
>
> Of course parylene would likely be the gold standard but it is not an
> option in this instance.
>
> I seem to recall that a past paper from Hunt/NPL supports the theory that
> just about all coatings are permeable to vapors . (~ also per 3-11G
> group)
>
> If that is truly the case not sure if it really matters which coating it
> is (not AR of course). Reason I am not willing to state that yet is I
> wonder if Ethylene Oxide would have any other detrimental effect on
> certain classes of coatings such as yellowing, embrittlement, etc.
>
> Any thoughts would be appreciated
>
>
> Rich Kraszewski
> Senior Staff Process Engineer
> Plexus Engineering Solutions
>
>
> * * * * * * * * CONFIDENTIALITY NOTICE * * * * * * * *
>
> This e-mail and any attachments are confidential from Plexus Corp. and may
> contain information which is privileged, confidential, and/or protected by
> non-disclosure agreements. They are intended solely for the use of the
> named addressee(s). . Any unauthorized use or disclosure may be
> unlawful. If you are not a named addressee, you must not use, disclose,
> retain or reproduce all or any part of the information contained in this
> e-mail or any attachments If you have received this transmission in error,
> please destroy it and notify us immediately by return e-mail or by calling +
> 1 888 208 9005.
>
|
|
|