Peter,
I don't believe there is anything in IPC-A-610 specific to this, but there are requirements in J-STD-001. See paragraph 4.18.3 "Partially Visible or Hidden Solder Connections"
Ben
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Peter Wong
Sent: Tuesday, June 6, 2017 4:25 PM
To: [log in to unmask]
Subject: EXTERNAL: [TN] Vertical fill
Hi everyone,
We have a conflict between inspectors. We have a through hole header where the destination side solder joints are partially hidden.
This is an IPC-A-610 Class 2 assembly and we are wondering what are the requirements for vertical fill and wetting on the destination side when you can't see them?
Thanks
Peter
________________________________
The enclosed documents are proprietary items to Silicon Forest Electronics' (SFE) customers. They shall not be reproduced nor disclosed for any purpose except as specified in writing from an authorized agent of SFE. These documents may contain data restricted for export by the International Traffic in Arms Regulations (ITAR) section of the Arms Export Control Act (or the Export Administration Act). Violators are subject to severe criminal penalties.
This e-mail, and any file attached to it, is meant only for the intended recipient of the transmission and may be a communication privileged by law. If you have received it in error, please notify the sender immediately and delete the original from your system. Any other use of this e-mail by you is strictly forbidden.
|
|
|