TECHNET Archives

June 2017

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Show All Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Subject:
From:
Richard Kraszewski <[log in to unmask]>
Reply To:
TechNet E-Mail Forum <[log in to unmask]>, Richard Kraszewski <[log in to unmask]>
Date:
Mon, 19 Jun 2017 21:19:36 +0000
Content-Type:
text/plain
Parts/Attachments:
text/plain (76 lines)
We have had best luck with 3M 401+

Rich  Kraszewski
Senior Staff Process Engineer
Plexus Engineering Solutions
Ship To - 2444 Schultz Dr. Neenah, WI 54957-2444
Mail To - P.O. Box 2444 Neenah, WI 54957-2444
Phone: (920) 969-6075
www.plexus.com/(NASDAQ PLXS)
[log in to unmask]


* * * * * * * * CONFIDENTIALITY NOTICE * * * * * * * *

This e-mail and any attachments are confidential from Plexus Corp. and may contain information which is privileged, confidential, and/or protected by non-disclosure agreements.  They are intended solely for the use of the named addressee(s).  .  Any unauthorized use or disclosure may be unlawful.  If you are not a named addressee, you must not use, disclose, retain or reproduce all or any part of the information contained in this e-mail or any attachments If you have received this transmission in error, please destroy it and notify us immediately by return e-mail or by calling + 1 888 208 9005.

-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Craig Sullivan
Sent: Monday, June 19, 2017 11:00 AM
To: [log in to unmask]
Subject: [TN] Conformal coat tape of acrylic

What masking tape is everyone using for Type AR coatings?

 

Long story short:

We used to use the St. Gobain M797 which was also known as Humiseal's HT-500. Due to numerous manufacturer issues, we stopped using it.

One of our customers spec'd in the blue 3m painter's tape and we have been using it successfully for a while.

We have some new assemblies where the 3m adhesion is terrible and am now back onto looking for a new tape, similar to what we all went through some 8 years ago.

 

Craig Sullivan

Manufacturing Engineer

IT Administrator

Phone: (607) 266-0480 x115

Fax: (607) 266-0482

Email: <mailto:[log in to unmask]> [log in to unmask]

Web: <http://www.mplinc.com/> www.mplinc.com

 

MPL, Inc.

41 Dutch Mill Road | Ithaca | NY | 14850

An ISO 9001:2008 Certified and ITAR Registered Company

IPC member since 2004

 

  _____

Confidentiality Notice:
This e-mail contains privileged and confidential information which is the property of MPL Incorporated, intended only for the use of the intended recipient(s). Unauthorized use or disclosure of this information is prohibited. If you are not an intended recipient, please immediately notify MPL Incorporated and destroy any copies of this email. Receipt of this e-mail shall not be deemed a waiver by MPL Incorporated of any privilege or the confidential nature of the information.

Export Control:
This message is intended only for the addressee and may contain information that is company confidential or privileged. Any technical data in this message may be exported only in accordance with the U.S. International Traffic in Arms Regulations (22 CFR Parts 120-130) or the Export Administration Regulations (15 CFR Parts 730-774). Unauthorized use is strictly prohibited and may be unlawful. If you are not the intended recipient, or the person responsible for delivering to the intended recipient, you should not read, copy, disclose or otherwise use this message. If you have received this email in error, please delete it, and advise the sender immediately.

 

 

 

ATOM RSS1 RSS2