Hello Brian,
Your point about the solutions being very different based on your premises
below
is correct, but you are also speaking of very small volume quantities.
Evaporation would be a major factor to consider in your error calculations
in each of those cases. In my world, I am dealing with, at minimum, a liter
of solution when I make it. So the evaporation is less noticeable, IMHO.
For mixing, I personally prefer volume to volume measurements over mass
because I believe them to be the most accurate. To that end, I have
estimated the specific gravity (SG) of the 75/25 mixture based on the CRC
values for each material and have built in a +/-5% tolerance for each to
account for
variation in the mixture. I have found, after years of doing this, that a
few degrees shift from 20 - 25 C
has very little affect on the SG measurement of the mixture. I
know this because I track both the SG and temperature every time I make a
"batch" and have not seen appreciable differences in the
SG mixture results.
Best regards,
Joe Russeau
-----Original Message-----
From: Brian Ellis
Sent: Thursday, June 29, 2017 7:53 AM
To: [log in to unmask]
Subject: Re: [TN] IPC definition of alcohol
Just a little question re mixtures of IPA and water. Let's say you want
a 75% mixture. Do you...
a) weigh 75 g of IPA and 25 g of H2O? If so, at what temperature for
each component?
b) measure 75 ml of IPA and add 25 ml of water? If so, at what
temperature for each component?
c) measure 75 ml of IPA and add water to make up to 100 ml? If so, at
what temperature for each component?
d) measure 25 ml of water and add IPA to make up to 100 ml? If so, at
what temperature for each component?
Assuming the temperature is the same for the two components (big if, in
many cases!), each of the four solutions above will be very different
from each other (of course, also applies to 50% solutions). The problem
is because mixtures of the two liquids do not form an ideal solution.
The loose structure of the water molecules leaves space for the tight
structure of the IPA molecules to fit in (simplified explanation - look
up wiki Ideal Solution.)
If you do a scientific test with each of the four mixtures, you will
find that the measured conductivity after injecting a known quantity of
a test solution will vary by up to 15%.
Just a thought...
Brian Ellis
On 29/06/2017 00:25, Joe Russeau wrote:
> Hello Rich,
>
> To the best of my knowledge, I am not aware of a statement to that
> affect in any IPC document that I have read. If there is such a
> statement, then I would say it is an erroneous one and needs to be
> addressed. There is HPLC grade IPA, which usually refers to 99.5% or
> higher purity. There is also Electronic-grade IPA, which has the same
> purity as HPLC. Then there is Technical grade IPA, which I believe is
> usually classified as anything above 90% purity. IPA is a chemical and
> its percentage of purity doesn't define whether or not it is still an
> "IPA", it's chemical formula defines that. The % only defines how much
> junk is left behind in the solvent. Now, there are IPC methods that
> deal with the percentage of the starting IPA, such as the ROSE and Ion
> Chromatography methods, and the reason is to minimize adding error into
> the measurement system that could skew the results for an actual
> sample. If there is a statement as you indicate below, can you ask
> whoever told you that which IPC document states such a thing? If not, I
> wonder if someone might have misread that part of the document
>
> Best Regards,
>
> Joe Russeau
>
>
>
> -----Original Message----- From: Richard Kraszewski
> Sent: Wednesday, June 28, 2017 4:48 PM
> To: [log in to unmask]
> Subject: [TN] IPC definition of alcohol
>
> I have been lead to believe that there is a definition within IPC
> documentation for IPA (isopropyl alcohol).
> That it defines that anything greater than "XX%" IPA shall be
> considered IPA.
>
> Any thoughts?
>
>
> Rich Kraszewski
> Senior Staff Process Engineer
> Plexus Engineering Solutions
> Ship To - 2444 Schultz Dr. Neenah, WI 54957-2444
> Mail To - P.O. Box 2444 Neenah, WI 54957-2444
> Phone: (920) 969-6075
> www.plexus.com/(NASDAQ PLXS)
> [log in to unmask]
>
>
> * * * * * * * * CONFIDENTIALITY NOTICE * * * * * * * *
>
> This e-mail and any attachments are confidential from Plexus Corp. and
> may contain information which is privileged, confidential, and/or
> protected by non-disclosure agreements. They are intended solely for
> the use of the named addressee(s). . Any unauthorized use or
> disclosure may be unlawful. If you are not a named addressee, you must
> not use, disclose, retain or reproduce all or any part of the
> information contained in this e-mail or any attachments If you have
> received this transmission in error, please destroy it and notify us
> immediately by return e-mail or by calling + 1 888 208 9005.
>
> ---
> This email has been checked for viruses by Avast antivirus software.
> https://www.avast.com/antivirus
>
|