You might try the Shercon line of green polyester tapes. They work well
with our acrylics.
https://www.caplugs.com/catalog/tapes-die-cuts.html
Doug Pauls
Principal Materials and Process Engineer
Rockwell Collins
On Mon, Jun 19, 2017 at 10:59 AM, Craig Sullivan <[log in to unmask]>
wrote:
> What masking tape is everyone using for Type AR coatings?
>
>
>
> Long story short:
>
> We used to use the St. Gobain M797 which was also known as Humiseal's
> HT-500. Due to numerous manufacturer issues, we stopped using it.
>
> One of our customers spec'd in the blue 3m painter's tape and we have been
> using it successfully for a while.
>
> We have some new assemblies where the 3m adhesion is terrible and am now
> back onto looking for a new tape, similar to what we all went through some
> 8
> years ago.
>
>
>
> Craig Sullivan
>
> Manufacturing Engineer
>
> IT Administrator
>
> Phone: (607) 266-0480 x115
>
> Fax: (607) 266-0482
>
> Email: <mailto:[log in to unmask]> [log in to unmask]
>
> Web: <http://www.mplinc.com/> www.mplinc.com
>
>
>
> MPL, Inc.
>
> 41 Dutch Mill Road | Ithaca | NY | 14850
>
> An ISO 9001:2008 Certified and ITAR Registered Company
>
> IPC member since 2004
>
>
>
> _____
>
> Confidentiality Notice:
> This e-mail contains privileged and confidential information which is the
> property of MPL Incorporated, intended only for the use of the intended
> recipient(s). Unauthorized use or disclosure of this information is
> prohibited. If you are not an intended recipient, please immediately notify
> MPL Incorporated and destroy any copies of this email. Receipt of this
> e-mail shall not be deemed a waiver by MPL Incorporated of any privilege or
> the confidential nature of the information.
>
> Export Control:
> This message is intended only for the addressee and may contain information
> that is company confidential or privileged. Any technical data in this
> message may be exported only in accordance with the U.S. International
> Traffic in Arms Regulations (22 CFR Parts 120-130) or the Export
> Administration Regulations (15 CFR Parts 730-774). Unauthorized use is
> strictly prohibited and may be unlawful. If you are not the intended
> recipient, or the person responsible for delivering to the intended
> recipient, you should not read, copy, disclose or otherwise use this
> message. If you have received this email in error, please delete it, and
> advise the sender immediately.
>
>
>
>
>
>
>
|
|
|