TECHNET Archives

June 2017

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
Date:
Fri, 9 Jun 2017 19:09:22 +0000
Reply-To:
TechNet E-Mail Forum <[log in to unmask]>, Ken Barton <[log in to unmask]>
Message-ID:
Subject:
From:
Ken Barton <[log in to unmask]>
MIME-Version:
1.0
In-Reply-To:
Content-Transfer-Encoding:
base64
Content-Type:
text/plain; charset="utf-8"
Parts/Attachments:
text/plain (1 lines)
Good stuff, much appreciated!



Ken Barton CID

Technical Designer,

Avionics HW

                    

Blue Origin, LLC                                                        

21218 76th Avenue S.

Kent, WA 98032 (253) 437-5625 x625

[log in to unmask]





-----Original Message-----

From: TechNet [mailto:[log in to unmask]] On Behalf Of Joyce Koo

Sent: Friday, June 09, 2017 12:04 PM

To: [log in to unmask]

Subject: Re: [TN] [EXTERNAL] [TN] Fw: rad hard



Go through official channel to get access to the database...and generate your own... pay special attention to which plant the device come from... (dash number, ), they may be  different even from same brand. E.g. Using different die attach with filler, after irradiation, it might become radioactive with long isotopes. Off line. Devil is in the details.  



Sent from my BlackBerry 10 smartphone.

  Original Message  

From: Ken Barton

Sent: Friday, June 9, 2017 14:47

To: [log in to unmask]

Reply To: TechNet E-Mail Forum

Subject: Re: [TN] [EXTERNAL] [TN] Fw: rad hard



Thank you!



Ken Barton CID

Technical Designer,

Avionics HW



Blue Origin, LLC 

21218 76th Avenue S.

Kent, WA 98032 (253) 437-5625 x625

[log in to unmask]





-----Original Message-----

From: TechNet [mailto:[log in to unmask]] On Behalf Of Joyce Koo

Sent: Friday, June 09, 2017 11:42 AM

To: [log in to unmask]

Subject: [EXTERNAL] [TN] Fw: rad hard



Sent from my BlackBerry 10 smartphone.

  Original Message  

From: [log in to unmask]

Sent: Friday, June 9, 2017 14:40

To: [log in to unmask]https://solarsystem.nasa.gov/docs/1_RHESE.pdf