Hi Bob,
Well, the next step down with Galden heat transfer fluids is the HT200
which has a boiling point of 200 C. 3M makes some 215 C. fluorinert, called
their FC70 if you can find it. Last time I looked was up close to $1,000 a
gallon...
Steve
On Sat, Apr 15, 2017 at 1:12 PM, Bob Wettermann <[log in to unmask]> wrote:
> All:
>
> We are running an experiment on the use of vapor phase reflow for a rework
> process due to the excessive warpage (confirmed by and quantified by Shadow
> Moire' measurements) of a specific component.We want to keep the
> temperature of the component, which is an Sn63 soldered component, as low
> as possible. The balance of the board is all soldered using a SAC305 alloy.
>
> We are "renting time" on a local company's VP reflow oven to run the
> experiments.
>
> Last week went over the DOE and the engineer who is responsible at the
> company that owns the vapor phase claims that they profile tin lead and
> lead-free boards using the same fluid in the bed and just adjust the time
> and heater conditions to get the right profile.
>
> I understood that you were to match the fluid to the solder alloy/liquidus
> temperature-right?
>
> Being used in the machine is the Solvay S 230 230°C for unleaded solder
> (e.g.. SnCuAg)
>
> Comments would be appreciated.
> --
> Bob Wettermann
> BEST Inc
> [log in to unmask]
> Cell: 847-767-5745
>
--
This email and any attachments are only for use by the intended
recipient(s) and may contain legally privileged, confidential, proprietary
or otherwise private information. Any unauthorized use, reproduction,
dissemination, distribution or other disclosure of the contents of this
e-mail or its attachments is strictly prohibited. If you have received this
email in error, please notify the sender immediately and delete the
original.
|
|
|