If you cannot justify a $60k+ investment, hiring an operator and/or a
chemist, then go with a 3rd party lab.
Delta Tg is a standard straightforward measurement.
On Thu, Mar 9, 2017 at 7:45 AM, <[log in to unmask]> wrote:
> Fellow TechNetters:
>
> Can anyone out there provide suggestion for a DSC models for PWB
> laminate cure analysis.
>
> Victor,
>
--
Bhanu Sood