MT also good.
http://www.mt.com/ca/en/home/products/Laboratory_Analytics_Browse/TA_Family_Browse/DSC.tabs.models-and-specs.html
> Vicotr,
> Try TA and Perkin Elmer for companies. Models will depend on what options
> you want.
>
> Regards,
> Bev
>
> -----Original Message-----
> From: TechNet [mailto:[log in to unmask]] On Behalf Of
> [log in to unmask]
> Sent: Thursday, March 09, 2017 7:46 AM
> To: [log in to unmask]
> Subject: [TN] Differential Scanning Calorimetry
>
> Fellow TechNetters:
>
> Can anyone out there provide suggestion for a DSC models for PWB
> laminate
> cure analysis.
>
> Victor,
>