Yup. Do it every day.
Essential tools are:
Reflow: Good prediction software and lots of patience
Wave: X-ray with oblique viewing.
Do brush up on hole fill requirements for thru-hole. Rev F changed it a little.
Ed Popielarski
Engineering Manager
970 NE 21st Ct.
Oak Harbor, Wa. 98277
Ph: 360-675-1322
Fx: 206-624-0695
Cl: 360-544-2289
"It's one kind of victory to slay a beast, move a mountain, and cross a chasm, but it's another kind altogether to realize that the beast, the mountain, and the chasm were of your own design."
https://goo.gl/maps/mMjg43rXeFB2
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Nutting, Phil
Sent: Thursday, March 30, 2017 10:57 AM
To: [log in to unmask]
Subject: [TN] circuit board layout optimization for manufacturing
Hi all,
Are there any standards or guidelines for how PCBs are laid out when dealing with small components in one area and large thermal mass components and ground planes in another area and being successful in wave soldering or reflow?
Phil Nutting | HVP Development Engineer | Excelitas Technologies Corp
Lab: +1 978.224.4332 | Office: +1 978.224.4152
35 Congress St, Salem, MA 01970 USA
[log in to unmask]<mailto:[log in to unmask]>
www.excelitas.com<http://www.excelitas.com/>
[Excelitas R_emailsig]
Please consider the environment before printing this e-mail.
________________________________
This email message and any attachments are confidential and proprietary to Excelitas Technologies Corp. If you are not the intended recipient of this message, please inform the sender by replying to this email or sending a message to the sender and destroy the message and any attachments. Thank you.
|
|
|