TECHNET Archives

March 2017

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
TechNet E-Mail Forum <[log in to unmask]>, Wayne Thayer <[log in to unmask]>
Date:
Mon, 20 Mar 2017 16:29:19 -0400
Reply-To:
TechNet E-Mail Forum <[log in to unmask]>, [log in to unmask]
Message-ID:
Subject:
From:
Joyce Koo <[log in to unmask]>
Content-Transfer-Encoding:
quoted-printable
In-Reply-To:
Content-Type:
text/plain; charset="iso-8859-1"
MIME-Version:
1.0
Parts/Attachments:
text/plain (131 lines)
and it is not repairable (unless you sand blast it... not nice)
> Parylene is a fine dielectric. It is just expensive and painful to apply
> (vacuum deposition so masking of where you don't want it needs to be much
> more aggressive than masking for spray or even dip).
>
> -----Original Message-----
> From: TechNet [mailto:[log in to unmask]] On Behalf Of Robert Kondner
> Sent: Monday, March 20, 2017 10:39 AM
> To: [log in to unmask]
> Subject: Re: [TN] WG: [TN] Screen On Insulation
>
> Hi,
>
>  Is the use of parylene NOT recommended as an insulating layer? It sure
> has a high dielectric strength.
>
> Does anyone have comments? I knid of like the parylene ide as it gets into
> all the itty bitty places.
>
> Bob
>
> -----Original Message-----
> From: TechNet [mailto:[log in to unmask]] On Behalf Of Theodore J. Tontis
> Sent: Monday, March 20, 2017 12:38 PM
> To: [log in to unmask]
> Subject: Re: [TN] WG: [TN] Screen On Insulation
>
> Coating is not to be used as an insulator. There is no guarantee that
> consistent coating thickness can be controlled meaning the ability to
> insulate/electrically isolate cannot be controlled.
>
> If the concern is the planar core shorting to the board, ask the supplier
> to place kapton tape under the core.
>
> All of our planar transformer drawings call out kapton on the bottom of
> the core for this very reason.
>
> Ted T
>
> -----Original Message-----
> From: TechNet [mailto:[log in to unmask]] On Behalf Of Robert Kondner
> Sent: Monday, March 20, 2017 11:06 AM
> To: [log in to unmask]
> Subject: Re: WG: [TN] Screen On Insulation
>
> Torsten,
>
>  Do you know how thick a parylene coating is? My recollection is pretty
> thin.
>
>  So I checked, very high dielectric strength, thickness typically under 1
> mil but it can be built up further with longer processing time.
>
> Any idea wat coating with parylene cost for a small batch of boards?
>
> Thanks,
> Bob Kondner
>
>
> -----Original Message-----
> From: TechNet [mailto:[log in to unmask]] On Behalf Of Torsten Hagge
> Sent: Monday, March 20, 2017 9:17 AM
> To: [log in to unmask]
> Subject: [TN] WG: [TN] Screen On Insulation
>
> Hi,
>
> cheap solution could be a 1mil kapton tape with the mention risk of air
> gaps, fine and cost expensive solution parylene HT  coating before placing
> the ferrite cores...
>
> Take care
> Torsten
>
>
>
> Best Regards
>
> KRISTRONICS GmbH
>
> Dipl.Ing. (FH) Torsten Hagge
> team leader HW development
> Gewerbegrund 5-9
> 24955 Harrislee
> Telefon +49 (0) 461 7741-624
> Telefax +49 (0) 461 7741-642
> [log in to unmask]
> www.kristronics.de
> Place of jurisdiction: Flensburg, commercial register: HRB 1433 FL
> CEO Dipl.-Ing. oec. Thormod Ohm
> VAD-Id DE 811182059
> Bank account: Deutsche Bank AG Flensburg, account 4216610, bank number
> 21570011
> IBAN: DE32 2157 0011 0421 6610 00, BIC: DEUT DE HH 215
>  Please consider the environment before printing this e-mail
>
>
>
> -----Ursprüngliche Nachricht-----
> Von: TechNet [mailto:[log in to unmask]] Im Auftrag von Robert Kondner
> Gesendet: Freitag, 17. März 2017 21:11
> An: [log in to unmask]
> Betreff: [TN] Screen On Insulation
>
> Hi,
>
>
>
> We have a PCB that turns out to require 2500VAC test for 60 seconds and we
> had some flash over on pads to vias. We also have a planar ferrite
> transformer with primary windings on one side.
>
>
>
> Does anyone know of a screen on insulation material that can be used to
> increase flash over voltages? I would like to get a 2 or 3 mils of
> material.
> My other option is to have a laser cut layer of isolation but that could
> leave air paths under the material.
>
>
>