TECHNET Archives

March 2017

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
TechNet E-Mail Forum <[log in to unmask]>, "Nutting, Phil" <[log in to unmask]>
Date:
Tue, 7 Mar 2017 13:03:48 -0600
Reply-To:
TechNet E-Mail Forum <[log in to unmask]>, Iulia Muntele <[log in to unmask]>
Message-ID:
Subject:
From:
Iulia Muntele <[log in to unmask]>
Content-Transfer-Encoding:
quoted-printable
In-Reply-To:
Content-Type:
text/plain; charset="UTF-8"
MIME-Version:
1.0
Parts/Attachments:
text/plain (82 lines)
I also wonder if you pour liquid nitrogen over it, if the top layer may
'pop off' due to mismatch...

On Tue, Mar 7, 2017 at 12:55 PM, Iulia Muntele <[log in to unmask]>
wrote:

> a handheld XRF may work faster with no need for material removal
>
> On Tue, Mar 7, 2017 at 12:52 PM, Nutting, Phil <[log in to unmask]
> > wrote:
>
>> I’ll have to see if we have an SEM.  It is very possible this pot had
>> SAC305 in it.  I can tell you it killed a carbide drill bit.
>>
>> From: David Hillman [mailto:[log in to unmask]]
>> Sent: Tuesday, March 07, 2017 1:50 PM
>> To: TechNet E-Mail Forum; Nutting, Phil
>> Subject: Re: [TN] grunge at bottom of tinning solder pot
>>
>> Hi Phil - what you have is an IMC which is more dense that solder so it
>> sank to the bottom. It may be FeSn which is pretty tough to remove.  Use
>> the SEM to figure out what IMC you have and then it may be possible to
>> dissolve it with another solder alloy (i.e. SAC305, etc.).
>>
>> Dave Hillman
>> Rockwell Collins
>> [log in to unmask]<mailto:david.hillman@rockw
>> ellcollins.com>
>>
>> On Tue, Mar 7, 2017 at 12:12 PM, Nutting, Phil <
>> [log in to unmask]<mailto:[log in to unmask]>> wrote:
>> I have two wire tinning solder pots that have not received the proper
>> day-to-day maintenance and now there is solid crud filling all but about ¼
>> of the crucible.  I have tried chiseling it out and drilling it out.  All I
>> end up with is dull tools, even carbide drills.
>>
>> Other than buying new solder pots or replacing the crucibles are there
>> any suggestions for removing this super hard stuff?
>>
>> Phil Nutting  |  HVP Development Engineer   |  Excelitas Technologies Corp
>>
>> Lab: +1 978.224.4332<tel:%2B1%20978.224.4332>   |  Office: +1
>> 978.224.4152<tel:%2B1%20978.224.4152>
>> 35 Congress St, Salem, MA  01970 USA
>> [log in to unmask]<mailto:[log in to unmask]<mailto:
>> [log in to unmask]>>
>> www.excelitas.com<http://www.excelitas.com><http://www.excelitas.com/>
>>
>>
>> [Excelitas R_emailsig]
>>
>>
>> Please consider the environment before printing this e-mail.
>> ________________________________
>> This email message and any attachments are confidential and proprietary
>> to Excelitas Technologies Corp. If you are not the intended recipient of
>> this message, please inform the sender by replying to this email or sending
>> a message to the sender and destroy the message and any attachments. Thank
>> you.
>>
>>
>

-- 
CONFIDENTIALITY
This e-mail message and any attachments thereto, is intended only for use 
by the addressee(s) named herein and may contain legally privileged and/or 
confidential information. If you are not the intended recipient of this 
e-mail message, you are hereby notified that any dissemination, 
distribution or copying of this e-mail message, and any attachments 
thereto, is strictly prohibited. If you have received this e-mail message 
in error, please immediately notify the sender and permanently delete the 
original and any copies of this email and any prints thereof.
ABSENT AN EXPRESS STATEMENT TO THE CONTRARY HEREINABOVE, THIS E-MAIL IS NOT 
INTENDED AS A SUBSTITUTE FOR A WRITING. Notwithstanding the Uniform 
Electronic Transactions Act or the applicability of any other law of 
similar substance and effect, absent an express statement to the contrary 
hereinabove, this e-mail message its contents, and any attachments hereto 
are not intended to represent an offer or acceptance to enter into a 
contract and are not otherwise intended to bind the sender, Sanmina 
Corporation (or any of its subsidiaries), or any other person or entity.

ATOM RSS1 RSS2