I assume you can turn on the pot and melt the solder, then scoop both the molten solder and the crud out, scrape it clean, fill it with fresh solder and send it out for analysis, if it passes continue production, update the maintenance schedule, and go from there.
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Nutting, Phil
Sent: Tuesday, March 07, 2017 12:13 PM
To: [log in to unmask]
Subject: [TN] grunge at bottom of tinning solder pot
I have two wire tinning solder pots that have not received the proper day-to-day maintenance and now there is solid crud filling all but about ¼ of the crucible. I have tried chiseling it out and drilling it out. All I end up with is dull tools, even carbide drills.
Other than buying new solder pots or replacing the crucibles are there any suggestions for removing this super hard stuff?
Phil Nutting | HVP Development Engineer | Excelitas Technologies Corp
Lab: +1 978.224.4332 | Office: +1 978.224.4152
35 Congress St, Salem, MA 01970 USA
[log in to unmask]<mailto:[log in to unmask]>
www.excelitas.com<http://www.excelitas.com/>
[Excelitas R_emailsig]
Please consider the environment before printing this e-mail.
________________________________
This email message and any attachments are confidential and proprietary to Excelitas Technologies Corp. If you are not the intended recipient of this message, please inform the sender by replying to this email or sending a message to the sender and destroy the message and any attachments. Thank you.
|
|
|