TECHNET Archives

February 2017

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
TechNet E-Mail Forum <[log in to unmask]>, Lee Hitchens <[log in to unmask]>
Date:
Tue, 28 Feb 2017 12:08:14 -0500
Reply-To:
TechNet E-Mail Forum <[log in to unmask]>, [log in to unmask]
Message-ID:
Subject:
From:
Joyce Koo <[log in to unmask]>
Content-Transfer-Encoding:
quoted-printable
In-Reply-To:
Content-Type:
text/plain; charset="iso-8859-1"
MIME-Version:
1.0
Parts/Attachments:
text/plain (25 lines)
no published data, but baking usually is better (1) surface moisture are
gone... and (2) cured some un-cured solder mask - oxygen rich surface -
that bond better for coating... (majority of the coating).  IMHO.
regards,
  jk
> Hi all
>
> I've recently been asked about baking pcbs before conformal coating and
> whether there is any quantified data on the effect on coating performance.
>
> Does anyone know of any public studies on this or can shed some light on
> its effectiveness beyond anecdotal experience ? I would be very grateful
> to
> you on this.
>
> Best Regards
>
> Dr Lee Hitchens
>