TECHNET Archives

February 2017

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
TechNet E-Mail Forum <[log in to unmask]>
Date:
Thu, 16 Feb 2017 21:57:26 +0000
Reply-To:
TechNet E-Mail Forum <[log in to unmask]>, Ed Popielarski <[log in to unmask]>
Message-ID:
Subject:
From:
Ed Popielarski <[log in to unmask]>
MIME-Version:
1.0
In-Reply-To:
Content-Transfer-Encoding:
base64
Content-Type:
text/plain; charset="utf-8"
Parts/Attachments:
text/plain (1 lines)
A new half-fractional element is used: bismuth nickel



Ed Popielarski

Engineering Manager





                               970 NE 21st Ct.

                              Oak Harbor, Wa. 98277



                              Ph: 360-675-1322

                              Fx: 206-624-0695

                              Cl: 360-544-2289







       “It's one kind of victory to slay a beast, move a mountain, and cross a chasm, but it's another kind altogether to realize that the beast, the mountain, and the chasm were of your own design.”

https://goo.gl/maps/mMjg43rXeFB2



-----Original Message-----

From: TechNet [mailto:[log in to unmask]] On Behalf Of Reuven Rokah

Sent: Thursday, February 16, 2017 1:25 PM

To: [log in to unmask]

Subject: Re: [TN] New Solder Alloy



No news with the elements tested...180 deg C is fine, reliability issues should be followed in years to come / aging tests



On Tue, Feb 14, 2017 at 7:19 PM, Vargas, Stephen M < [log in to unmask]> wrote:



> Got news of this from a colleague. Interesting... would love to hear 

> comments from the TechNet group.

>

> http://news.lenovo.com/news-releases/lenovo-announces-

> breakthrough-innovative-pc-manufacturing-process.htm

>

> Regards,

> Steve Vargas

>







-- 



Best Regards,



*Reuven Rokah*



Mobile: 972-52-6012018

Tel:        972-3-9360688

Fax:          15339360688

<http://www.rokah-technologies.com/>[log in to unmask]

[log in to unmask]

www.rokah-technologies.com

The exclusive Israeli agent of:

http://www.greensofttech.com/



This e-mail message is intended for the recipient only and contains information which is CONFIDENTIAL and which may be proprietary of Rokah Technologies. If you have received this transmission in error, please inform me by e-mail, phone or fax, and then please delete all of the original files and all other copies exist.