DESIGNERCOUNCIL Archives

December 2016

DesignerCouncil@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Show All Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Subject:
From:
Jack Olson <[log in to unmask]>
Reply To:
(Designers Council Forum)
Date:
Mon, 19 Dec 2016 10:55:39 -0600
Content-Type:
text/plain
Parts/Attachments:
text/plain (158 lines)
*Kitty*,
so when you say "vias filled with soldermask and covered"
the "*and covered*" part is the adhesive?
Sorry to ask for more clarification, but I'm really interested in this.

*All,*
I inquired about the bare board quote, wondering how significant this
decision is.
My engineers are saying the bare board fabricator wants to add 25% for this
process
which in our case is over FIFTY DOLLARS PER BOARD!!!
seriously?
Can anyone share approximately what they have paid for filled vias?

(and to make sure I understood other responses:
plugged vias are not guaranteed 100%, right?
I think we need 100% because if a solder bump pokes through our thermal
insulating pad, the circuit could short out to the aluminum housing.)

thanks again,
Jack

On Mon, Dec 19, 2016 at 9:17 AM, Hines, Kitty <[log in to unmask]>
wrote:

> Hi Jack-
>
> We have the vias filled with solder mask and covered (not ‘TENTED’).
> We’re not paying for a secondary process.  Some vias will either not get
> fully filled, or will open during reflow.  So as others have also
> commented, vias will allow solder to wick during the wave process; the glue
> stops that from happening.  The only added cost we have is for extra glue.
>
> Kitty
>
>
>
>
>
> *From:* Jack Olson [mailto:[log in to unmask]]
> *Sent:* Monday, December 19, 2016 8:34 AM
> *To:* (Designers Council Forum) <[log in to unmask]>; Hines, Kitty <
> [log in to unmask]>
> *Subject:* Re: [DC] Plugging Thermal Via Holes with Soldermask?
>
>
>
> Hi Kitty,
>
>
>
> thanks for the interesting idea! I have never heard of that.
>
> We don't use wave soldering anymore, so we have cut the "adhesive" process
> out of the equation,
>
>
>
> What I don't understand is why you add adhesive dots on those vias if they
> are already filled and tented?
>
> (I could see using that method to AVOID the filling process)
>
>
>
> just curious,
>
> Jack
>
>
>
> On Thu, Dec 15, 2016 at 1:55 PM, Hines, Kitty <[log in to unmask]>
> wrote:
>
> Hi Jack,
> We have been struggling with the same problem.  We started adding a
> geometry to the glue stencil that will allow the glue to cover those bottom
> side vias.  The boards go thru reflow without wicking any solder thru.  The
> Fab drawing also calls out those vias to be "FULLY FILLED AND COVERED WITH
> SOLDER MASK ON SINGLE-SIDE ONLY (BOTTOM) PER IPC-4761, TYPE VI (a)."  Any
> solder balls in the hole will melt in the reflow ovens, and the glue stops
> solder from wicking up during the solder wave process.  So far, this has
> been working for us.  Do you see problems with this method?
>
>
>
>
> -----Original Message-----
> From: DesignerCouncil [mailto:[log in to unmask]] On Behalf Of Jack
> Olson
> Sent: Thursday, December 15, 2016 10:10 AM
> To: [log in to unmask]
> Subject: [DC] Plugging Thermal Via Holes with Soldermask?
>
> I'm looking at the various options for tenting/plugging/capping vias in
> IPC-4761 (Via Protection Guidelines). None of the options seem to address
> the thermal vias in power pads.
> We are trying to:
> 1) have a solderable pad, apply paste on that side (of course)
> 2) prevent solder from creating bumps on the heatsink side (of course)
> 3) avoid the cost of plugging/capping
>
> IPC-4671 states that all forms of one-sided via protection are NOT
> RECOMMENDED.
>
> So here's the question - I know I have seen a picture of a thermal pad in
> an IPC document where I could see vias with green mask material in them on
> the paste side (the component side), but the green stuff was only in the
> holes, which left the thermal pad exposed for soldering.
> I don't think this would be called TENTING because there's no mask on the
> pad. but is this an acceptable practice? Can I instruct a bare board
> fabricator to put mask in holes from the top side, but keep the pad clear?
> (I can't remember where I saw the picture!)
>
> If that's NOT an accepted practice, is there a way to design the hole big
> enough to plate but small enough to prevent solder flowing through the
> other side of the board? I couldn't find a discussion of that in the
> TechNet Archives
>
> thanks,
> Jack
>
> ------------------------------------------------------------
> ---------------------
> DesignerCouncil Mail List provided as a free service by IPC using LISTSERV
> 16.0.
> To unsubscribe, send a message to [log in to unmask] with following text in
> the BODY (NOT the subject field): SIGNOFF DesignerCouncil.
> To temporarily stop/(restart) delivery of DesignerCouncil send: SET
> DesignerCouncil NOMAIL/(MAIL) For additional information, or contact Keach
> Sasamori at [log in to unmask] or 847-615-7100 ext.2815
> ------------------------------------------------------------
> ---------------------
>
> ------------------------------------------------------------
> ---------------------
> DesignerCouncil Mail List provided as a free service by IPC using LISTSERV
> 16.0.
> To unsubscribe, send a message to [log in to unmask] with following text in
> the BODY (NOT the subject field): SIGNOFF DesignerCouncil.
> To temporarily stop/(restart) delivery of DesignerCouncil send: SET
> DesignerCouncil NOMAIL/(MAIL)
> For additional information, or contact Keach Sasamori at [log in to unmask]
> or 847-615-7100 ext.2815
> ------------------------------------------------------------
> ---------------------
>
>
>

---------------------------------------------------------------------------------
DesignerCouncil Mail List provided as a free service by IPC using LISTSERV 16.0.
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF DesignerCouncil.
To temporarily stop/(restart) delivery of DesignerCouncil send: SET DesignerCouncil NOMAIL/(MAIL)
For additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
---------------------------------------------------------------------------------

ATOM RSS1 RSS2