TECHNET Archives

December 2016

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
TechNet E-Mail Forum <[log in to unmask]>
Date:
Wed, 14 Dec 2016 16:43:10 +0000
Reply-To:
TechNet E-Mail Forum <[log in to unmask]>, Ioan Tempea <[log in to unmask]>
Message-ID:
Subject:
From:
Ioan Tempea <[log in to unmask]>
Content-Transfer-Encoding:
base64
In-Reply-To:
Content-Type:
text/plain; charset="utf-8"
MIME-Version:
1.0
Parts/Attachments:
text/plain (1 lines)
Thanks Dave,



I knew you guys were doing a good job in those committees!



Anything on wire pull, except Dage?



Best regards,



Ioan



De : David Hillman [mailto:[log in to unmask]]

Envoyé : Wednesday, December 14, 2016 10:59 AM

À : TechNet E-Mail Forum; Ioan Tempea

Objet : Re: [TN] Mechanical test equipment for MIL-883 methods 2003 and 2004



Hello Ioan - look in the back of the IPC JSTD 002 specification, Appendix E. There is solderability equipment information listed there in that Informative Annex.



Dave Hillman

Rockwell Collins

IPC-JSTD-002 chairman



On Wed, Dec 14, 2016 at 8:14 AM, Ioan Tempea <[log in to unmask]<mailto:[log in to unmask]>> wrote:

Dear Technos,



I need to test solderability (per J-STD-002 and method 2003, test B, of the 883) and lead integrity (method 2004 condition D of the 883) for leadless components.



Can you, please, suggest equipment for :



*         Steam aging



*         Solder bath dipping



*         Wire pull; this one is for method 2004, I wonder if anybody is using regular wire pulling machine (normally used for wire bonds) for this task.



Thank you,



Ioan Tempea, P. Eng.

Manufacturing Engineer, Satellite Systems



[cid:[log in to unmask]]



MacDonald, Dettwiler and Associates Corporation, 21025 Trans-Canada Highway, Ste-Anne-de-Bellevue, QC, Canada H9X 3R2

Tel: +1-514-457-2150 x3556<tel:%2B1-514-457-2150%20x3556>

www.mdacorporation.com<http://www.mdacorporation.com><http://www.mdacorporation.com/>



This e-mail, and any attachments, are intended solely for the use of the intended recipient(s) and may contain legally privileged, proprietary and/or confidential information. Any use, disclosure, dissemination, distribution or copying of this e-mail and any attachments for any purposes that have not been specifically authorized by the sender is strictly prohibited. If you are not the intended recipient, please immediately notify the sender by reply e-mail and permanently delete all copies and attachments. This email is for informational purposes only and shall not be interpreted to authorize or conclude a binding agreement between MDA and any other party unless this email contains or is accompanied by an express written confirmation of MDA's intention to enter into a binding agreement, such confirmation shall only be provided by an authorized representative of MDA.




ATOM RSS1 RSS2