TECHNET Archives

November 2016

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
TechNet E-Mail Forum <[log in to unmask]>
Date:
Tue, 1 Nov 2016 14:53:37 +0000
Reply-To:
TechNet E-Mail Forum <[log in to unmask]>, "Giamis, Andy" <[log in to unmask]>
Message-ID:
Subject:
From:
"Giamis, Andy" <[log in to unmask]>
MIME-Version:
1.0
In-Reply-To:
Content-Transfer-Encoding:
base64
Content-Type:
text/plain; charset="utf-8"
Parts/Attachments:
text/plain (1 lines)
Hi again Victor,

Browsing the internet a little deeper, I found several quirky cat videos and then this below regarding hard gold versus soft gold.  The video states that hard gold can be plated through an immersion process.



https://www.youtube.com/watch?v=bB-SgPE4PGw



Now, back to the cat videos...







-----Original Message-----

From: TechNet [mailto:[log in to unmask]] On Behalf Of Giamis, Andy

Sent: Tuesday, November 01, 2016 9:45 AM

To: [log in to unmask]

Subject: Re: [TN] Test



Hi Victor,

The great and all-knowing Wikipedia says hard gold often contains a small amount of cobalt or nickel.  

I am also not an expert, but I believe hard gold is an electrolytic process.  Although the electrolytic process can be stopped any time, typically target thicknesses are considerably thicker (30 micro-inches or more).  If you are looking at 5 micro-inches, I'd guess it is immersion gold.  The best action is to ask the supplier.  If that's not an option, try EDS looking for cobalt.  That's no guarantee, but positive results for cobalt would be informative.  5 micro-inches would be too thin to look for nickel.  Good luck.



Did I pass the test?





-----Original Message-----

From: TechNet [mailto:[log in to unmask]] On Behalf Of [log in to unmask]

Sent: Tuesday, November 01, 2016 7:19 AM

To: [log in to unmask]

Subject: Re: [TN] Test



Fellow TechNetters:



   I did not receive a response the FIRST time .   therefore I pose the inquiry once again.



“Is there a test or method to determine if gold plating is hard gold or ENIG?     XRF will determine thickness of gold but will not verify plating process.   I am working with a measurement of 5 micro inches of gold.”



Victor,



-----Original Message-----

From: TechNet [mailto:[log in to unmask]] On Behalf Of David Hillman

Sent: Tuesday, November 01, 2016 7:14 AM

To: [log in to unmask]

Subject: Re: [TN] Test



I don't know about the rest of the folks but I received an A+ and its rumored  you received a C-



Dave



On Tue, Nov 1, 2016 at 7:09 AM, Douglas Pauls < [log in to unmask]> wrote:



> And what percentage of our grade is this test?

>

>

> Doug Pauls

> Principal Materials and Process Engineer Rockwell Collins

>

> On Mon, Oct 31, 2016 at 9:17 AM, Vadim Matveyev 

> <[log in to unmask]>

> wrote:

>

> > Test

> >

>