Gents/Ladies:
This would be confirming gold plating thickness after repair using a brush
plating technique. Repair thickness is a function of many variables....
I was looking for an instrument to verify that would be cost effective as
it is for this single use.
Bob/BEST
On Tue, Oct 18, 2016 at 8:37 AM, Bev Christian <[log in to unmask]>
wrote:
> XRF
>
> Bev
>
> Sent from my BlackBerry 10 smartphone on the Bell network.
> Original Message
> From: Bob Wettermann
> Sent: Tuesday, October 18, 2016 9:28 AM
> To: [log in to unmask]
> Reply To: TechNet E-Mail Forum
> Subject: [TN] Measuring Gold Thickness
>
> Outside of x-sectional measurements for QA. can someone please share their
> favorite method/instrument for measuring gold thicknesses on PCBs?
>
> Thanks
>
> Bob/BEST
>
--
Bob Wettermann
BEST Inc
[log in to unmask]
Cell: 847-767-5745