They do have a low VOC version that we have used before as well.
Lloyd Duso
Plant Manager
Diamond-MT
(814) 535-3505
www.Diamond-mt.com
On Wed, Oct 5, 2016 at 11:08 AM, Wayne Thayer - EXT <[log in to unmask]
> wrote:
> Isn't that stuff about half toluene?
>
> Really--I love 1-2577 too, but won't it cause all of the "VOCs" alarms in
> the county to go off at once?
>
> Wayne Thayer
>
> -----Original Message-----
> From: TechNet [mailto:[log in to unmask]] On Behalf Of lduso - Diamond-MT.com
> Sent: Wednesday, October 05, 2016 7:54 AM
> To: [log in to unmask]
> Subject: Re: [TN] Silicone Conformal Coating supplier
>
> 90% of our customers (DOD & commercial) call out Dow 1-2577. A good all
> around SR that is extremely easy to apply, t/u, rework and has a very quick
> "dry" time of a mere 20 minutes @ room temp. Others are MG Chemicals and
> Humiseal.
>
> Lloyd Duso
> Plant Manager
> Diamond-MT
> (814) 535-3505
> www.Diamond-mt.com
>
> On Wed, Oct 5, 2016 at 10:48 AM, Stadem, Richard D. <
> [log in to unmask]> wrote:
>
> > I have a client who needs to qualify a silicone coating, either an
> > oven cure or UV cure coating. I am looking for a good supplier or
> distributor.
> > If any of you coating experts would care to share your favorites with
> > me, I would greatly appreciate it, as I am not an expert on sources of
> > coatings (best pricing, service, stocking, etc.) Feel free to contact
> > me directly by answering this email.
> > Thanks for any info you feel comfortable sharing.
> > dean
> >
>
|