TECHNET Archives

October 2016

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
TechNet E-Mail Forum <[log in to unmask]>
Date:
Tue, 18 Oct 2016 09:00:36 -0500
Reply-To:
TechNet E-Mail Forum <[log in to unmask]>, Bob Wettermann <[log in to unmask]>
Subject:
From:
Bob Wettermann <[log in to unmask]>
Message-ID:
In-Reply-To:
Content-Type:
text/plain; charset="UTF-8"
MIME-Version:
1.0
Parts/Attachments:
text/plain (42 lines)
Gents/Ladies:

This would be confirming gold plating thickness after repair using a brush
plating technique. Repair thickness is a function of many variables....

I was looking for an instrument to verify that would be cost effective as
it is for this single use.


Bob/BEST

On Tue, Oct 18, 2016 at 8:37 AM, Bev Christian <[log in to unmask]>
wrote:

> XRF
>
> Bev
>
> Sent from my BlackBerry 10 smartphone on the Bell network.
>   Original Message
> From: Bob Wettermann
> Sent: Tuesday, October 18, 2016 9:28 AM
> To: [log in to unmask]
> Reply To: TechNet E-Mail Forum
> Subject: [TN] Measuring Gold Thickness
>
> Outside of x-sectional measurements for QA. can someone please share their
> favorite method/instrument for measuring gold thicknesses on PCBs?
>
> Thanks
>
> Bob/BEST
>



-- 