TECHNET Archives

October 2016

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Show All Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Subject:
From:
Larry Dzaugis <[log in to unmask]>
Reply To:
TechNet E-Mail Forum <[log in to unmask]>, Larry Dzaugis <[log in to unmask]>
Date:
Mon, 17 Oct 2016 12:09:30 -0400
Content-Type:
text/plain
Parts/Attachments:
text/plain (19 lines)
It moves around based on process.

Pin in Paste is the topside/component side.

Selective solder is the side opposite the component.

Rare hand soldering for components only accessible from the top side, not
the preferred situation for DFM.
Select components in module assemblies come to mind.
Some designers do not accept sockets.

Inspection callout should include the situation so that the Inspector does
not reject valid joints.

Had large problem when selective solder connector went to pin in paste with
Inspectors rejecting good joints.