We use Shin-Etsu KE-3421, it is a condensation/moisture cure, tack free after 5 minutes or so, full cure in about 48 hours.
David Bealer
SMT Department Manager
office 800-637-2645 x6022 cell 217-474-8760
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Douglas Pauls
Sent: Wednesday, October 5, 2016 10:16 AM
To: [log in to unmask]
Subject: Re: [TN] Silicone Conformal Coating supplier
Dean,
We use Dow Corning 1-2577 as our approved silicone and it has always worked well for us. It is about 20-30% toluene, so it is a VOC, but if memory serves, there are low VOC versions of 1-2577 out there. While it does have a relatively quick tack time, you may want to bake it a while to drive the cure reaction and improve adhesion.
Doug Pauls
Principal Materials and Process Engineer Rockwell Collins
On Wed, Oct 5, 2016 at 10:08 AM, Wayne Thayer - EXT <[log in to unmask]
> wrote:
> Isn't that stuff about half toluene?
>
> Really--I love 1-2577 too, but won't it cause all of the "VOCs" alarms
> in the county to go off at once?
>
> Wayne Thayer
>
> -----Original Message-----
> From: TechNet [mailto:[log in to unmask]] On Behalf Of lduso -
> Diamond-MT.com
> Sent: Wednesday, October 05, 2016 7:54 AM
> To: [log in to unmask]
> Subject: Re: [TN] Silicone Conformal Coating supplier
>
> 90% of our customers (DOD & commercial) call out Dow 1-2577. A good
> all around SR that is extremely easy to apply, t/u, rework and has a
> very quick "dry" time of a mere 20 minutes @ room temp. Others are MG
> Chemicals and Humiseal.
>
> Lloyd Duso
> Plant Manager
> Diamond-MT
> (814) 535-3505
> www.Diamond-mt.com
>
> On Wed, Oct 5, 2016 at 10:48 AM, Stadem, Richard D. <
> [log in to unmask]> wrote:
>
> > I have a client who needs to qualify a silicone coating, either an
> > oven cure or UV cure coating. I am looking for a good supplier or
> distributor.
> > If any of you coating experts would care to share your favorites
> > with me, I would greatly appreciate it, as I am not an expert on
> > sources of coatings (best pricing, service, stocking, etc.) Feel
> > free to contact me directly by answering this email.
> > Thanks for any info you feel comfortable sharing.
> > dean
> >
>
|