Dave is absolutely right. I'd also suggest to do a better planar SEM/EDS. That's what we normally do for our customers in similar cases.
Regards
Vladimir
SENTEC
Sent from my BlackBerry 10 smartphone on the Rogers network.
Original Message
From: David Hillman
Sent: Tuesday, October 18, 2016 11:27
To: [log in to unmask]
Reply To: TechNet E-Mail Forum
Subject: Re: [TN] Something oxidized on pin surface
My recommendation is to conduct a metallurgical cross-section (which is
going to not be a simple task). There are a number of possible root causes
but understanding if there is a defect in the base material (your CuSn6) or
a defect in the plating structures is going to only be resolved by a
cross-sectional analysis.
Dave Hillman
Rockwell Collins
[log in to unmask]
On Tue, Oct 18, 2016 at 6:31 AM, Deng RongJun <[log in to unmask]> wrote:
> Hello All,
>
> I have got a problem that about pin insertion on PCB. It seems something
> oxidized on pin surface and will effect soldering at customer site, and
> this been found several month later after SMT assembly.
> Pin base material is CuSn6, and plating is: 1-2um Ni under 3-5um Sn 100.
> What is problem on pin surface? Any one of you have experience on this case?
>
> Pictures and SEM result:
> https://goo.gl/photos/GkZGsjRCQj16BW5V8
>
>
>
>
> Best regards
>
> Deng
>
|
|
|