TECHNET Archives

October 2016

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
TechNet E-Mail Forum <[log in to unmask]>, Douglas Pauls <[log in to unmask]>
Date:
Wed, 5 Oct 2016 11:21:30 -0400
Reply-To:
TechNet E-Mail Forum <[log in to unmask]>, "lduso - Diamond-MT.com" <[log in to unmask]>
Subject:
From:
"lduso - Diamond-MT.com" <[log in to unmask]>
Message-ID:
In-Reply-To:
Content-Type:
text/plain; charset="UTF-8"
MIME-Version:
1.0
Parts/Attachments:
text/plain (71 lines)
Another factor is that the fluorescence is not well dispersed so it does
not resemble a very smooth color like 1B31. It will be mottled under the
light but it is easy to see under white light.

Lloyd Duso
Plant Manager
Diamond-MT
(814) 535-3505
www.Diamond-mt.com

On Wed, Oct 5, 2016 at 11:15 AM, Douglas Pauls <
[log in to unmask]> wrote:

> Dean,
> We use Dow Corning 1-2577 as our approved silicone and it has always worked
> well for us.  It is about 20-30% toluene, so it is a VOC, but if memory
> serves, there are low VOC versions of 1-2577 out there.  While it does have
> a relatively quick tack time, you may want to bake it a while to drive the
> cure reaction and improve adhesion.
>
>
> Doug Pauls
> Principal Materials and Process Engineer
> Rockwell Collins
>
> On Wed, Oct 5, 2016 at 10:08 AM, Wayne Thayer - EXT <
> [log in to unmask]
> > wrote:
>
> > Isn't that stuff about half toluene?
> >
> > Really--I love 1-2577 too, but won't it cause all of the "VOCs" alarms in
> > the county to go off at once?
> >
> > Wayne Thayer
> >
> > -----Original Message-----
> > From: TechNet [mailto:[log in to unmask]] On Behalf Of lduso -
> Diamond-MT.com
> > Sent: Wednesday, October 05, 2016 7:54 AM
> > To: [log in to unmask]
> > Subject: Re: [TN] Silicone Conformal Coating supplier
> >
> > 90% of our customers (DOD & commercial) call out Dow 1-2577. A good all
> > around SR that is extremely easy to apply, t/u, rework and has a very
> quick
> > "dry" time of a mere 20 minutes @ room temp. Others are MG Chemicals and
> > Humiseal.
> >
> > Lloyd Duso
> > Plant Manager
> > Diamond-MT
> > (814) 535-3505
> > www.Diamond-mt.com
> >
> > On Wed, Oct 5, 2016 at 10:48 AM, Stadem, Richard D. <
> > [log in to unmask]> wrote:
> >
> > > I have a client who needs to qualify a silicone coating, either an
> > > oven cure or UV cure coating. I am looking for a good supplier or
> > distributor.
> > > If any of you coating experts would care to share your favorites with
> > > me, I would greatly appreciate it, as I am not an expert on sources of
> > > coatings (best pricing, service, stocking, etc.) Feel free to contact
> > > me directly by answering this email.
> > > Thanks for any info you feel comfortable sharing.
> > > dean
> > >
> >
>