TECHNET Archives

September 2016

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Show All Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Subject:
From:
Mumtaz Bora <[log in to unmask]>
Reply To:
TechNet E-Mail Forum <[log in to unmask]>, Mumtaz Bora <[log in to unmask]>
Date:
Tue, 6 Sep 2016 19:16:16 +0000
Content-Type:
text/plain
Parts/Attachments:
text/plain (1 lines)
Hi Blair, I suggest you take a good and the cloudy unit and EDX to see if there are any corrosive elements such as Chlorine, Sulphur etc.



-----Original Message-----

From: TechNet [mailto:[log in to unmask]] On Behalf Of Blair Hogg

Sent: Friday, September 02, 2016 7:45 AM

To: [log in to unmask]

Subject: [TN] Chromate coatings



Hi Technetters! Getting ready for the long weekend (at least here in the US)?



I'm looking for some advice on chromate coatings. We produce a phone for mining applications, which uses a battery held in by a bracket. The bracket is chromate coated.



The most recent batch of brackets sent out to the coating house came back with a cloudy appearance to the coating. Apparently something hiccupped in their process. The process can't be repeated, so we either scrap the parts and make new ones, or use them as is. Problem is, I don't know if the cloudy appearance will affect the corrosion protection properties. Any chromate experts out there that can offer any advice on this?



Thanks,

Blair

CONFIDENTIALITY NOTE: The information transmitted, including attachments, is intended only for the person(s) or entity to which it is addressed and may contain confidential and/or privileged material. Any review, retransmission, dissemination or other use of, or taking of any action in reliance upon this information by persons or entities other than the intended recipient is prohibited. If you received this in error, please contact the sender and destroy any copies of this information.