TECHNET Archives

September 2016

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
TechNet E-Mail Forum <[log in to unmask]>, Bev Christian <[log in to unmask]>
Date:
Mon, 19 Sep 2016 16:57:52 -0500
Reply-To:
TechNet E-Mail Forum <[log in to unmask]>, David Hillman <[log in to unmask]>
Subject:
From:
David Hillman <[log in to unmask]>
Message-ID:
In-Reply-To:
<701479EEB584478C96F66CA487045F11@bev1a0f3c0a9bc>
Content-Type:
text/plain; charset="UTF-8"
MIME-Version:
1.0
Parts/Attachments:
text/plain (23 lines)
DSC - good on qualifying organics and characterizing unknown materials on
pwas. And yes, I wanted to throw TGA in the mix!

Dave Hillman
Rockwell Collins
[log in to unmask]

On Mon, Sep 19, 2016 at 4:04 PM, Bev Christian <[log in to unmask]>
wrote:

> TechNetters,
> If you had the choice of getting ONE of:
> 1) TMA
> 2) DMA
> 3) DSC
>
> And $ was not an issue, which would you chose and WHY?  Please, no "it
> depends" answers and no, you can't throw TGA into the mix.
>
> Regards,