TECHNET Archives

August 2016

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Show All Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Subject:
From:
Bev Christian <[log in to unmask]>
Reply To:
TechNet E-Mail Forum <[log in to unmask]>, Bev Christian <[log in to unmask]>
Date:
Mon, 1 Aug 2016 12:08:15 -0400
Content-Type:
text/plain
Parts/Attachments:
text/plain (20 lines)
Graham
2.3.39C CANCELLED.  This is the only one that I am familiar with.  What is
your problem/issue you are trying to solve?
Regards,
Bev

-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Graham Naisbitt
Sent: Monday, August 01, 2016 11:57 AM
To: [log in to unmask]
Subject: [TN] FTIR

Hello fellow Techies,

Do any of you know if there is a test method in IPC for FTIR?

Thanks in advance

Graham Naisbitt