TECHNET Archives

August 2016

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Show All Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Subject:
From:
John Maxwell <[log in to unmask]>
Reply To:
TechNet E-Mail Forum <[log in to unmask]>, John Maxwell <[log in to unmask]>
Date:
Thu, 25 Aug 2016 15:23:48 -0400
Content-Type:
text/plain
Parts/Attachments:
text/plain (14 lines)
Victor,
The short answer is no color change is expected but if the part is experiencing internal heating then all bets are off.

Regards,

John Maxwell
> On Aug 25, 2016, at 2:59 PM, Victor Hernandez <[log in to unmask]> wrote:
> 
> Fellow TechNetters:
> 
>   During the service life of a ceramic capacitor will the ceramic material color change in color due to normal usage?   How about if the circuit draws too much current, overheating condition/leakage.
> 
> Victor,