TECHNET Archives

July 2016

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
TechNet E-Mail Forum <[log in to unmask]>, Steve Gregory <[log in to unmask]>
Date:
Thu, 28 Jul 2016 18:12:03 -0400
Reply-To:
TechNet E-Mail Forum <[log in to unmask]>, Yuan-chia Joyce Koo <[log in to unmask]>
Message-ID:
Subject:
From:
Yuan-chia Joyce Koo <[log in to unmask]>
Content-Transfer-Encoding:
7bit
In-Reply-To:
Content-Type:
text/plain; charset="US-ASCII"; delsp=yes; format=flowed
MIME-Version:
1.0 (Apple Message framework v753.1)
Parts/Attachments:
text/plain (159 lines)
opps, too quick... if you get a diode...wb could be a problem...
On Jul 28, 2016, at 5:03 PM, Steve Gregory wrote:

> Hi Joyce!
>
> Yep, as far as I can tell. There isn't much of a datasheet for the  
> relays
> that we are using, but it shares the same vibration and shock specs  
> as the
> Teledyne relays, so that tells me that they are very similar:
>
> http://www.te.com/commerce/DocumentDelivery/DDEController? 
> Action=srchrtrv&DocNm=PRMAC-26X&DocType=DS&DocLang=English
>
> Steve
>
>
>
> On Thu, Jul 28, 2016 at 2:18 PM, Joyce Koo <[log in to unmask]> wrote:
>
>> something similar to this internally?  if there are wire bonds  
>> connect to
>> the transient suppression diode, or some other tricky  
>> interconnect, it
>> might be...'
>> http://www.teledynerelays.com/pdf/electromechanical/432.pdf
>> steve, do you have internal construction x-ray image? TO-5 is very  
>> strong
>> seal using glass, interconnect using spot weld to the leads may  
>> not be
>> easy to damaged, depend upon how it constructed.  my 1.4 cents.
>> http://www.teledynerelays.com/pdf/electromechanical/432.pdf
>>
>>  jk
>> http://www.teledynerelays.com/pdf/electromechanical/432.pdf
>>> Steve,
>>> Do they have PROOF that bending the leads cause damage?
>>> Bev
>>>
>>> -----Original Message-----
>>> From: TechNet [mailto:[log in to unmask]] On Behalf Of Steve Gregory
>>> Sent: Thursday, July 28, 2016 11:12 AM
>>> To: [log in to unmask]
>>> Subject: [TN] Prepping TO-5 can style Relay...
>>>
>>> Hi All,
>>>
>>> We're building a board for a customer that uses a 8-lead TO-5 style
>> relay.
>>> The footprint on the board requires that the leads are spread out  
>>> to a
>>> larger diameter circle than what diameter is when they come out  
>>> of the
>>> body
>>> at the bottom of the relay. Here's the information for one of the  
>>> relays,
>>> there are three others that are the same style:
>>>
>>>
>> http://www.digikey.com/product-search/en? 
>> lang=en&site=us&WT.z_cid=ref_findch
>>> ips_standard&mpart=PRMAC-26X
>>>
>>> So we have a Simonds CLP274 lead processor with a die that  
>>> matches the
>>> footprint on the PCB:
>>>
>>> http://stevezeva.homestead.com/Simonds_CLP274.jpg
>>>
>>> We insert the part which spreads the leads out, then step on the  
>>> pedal
>> and
>>> a guillotine style blade shears the leads off. I've used the prep  
>>> unit
>>> many, many time before at previous employers without issues. The  
>>> customer
>>> is saying that prepping the leads in this unit is damaging the  
>>> relay. So
>>> now we are to pot the leads before prepping them with a 2-part epoxy
>> using
>>> a tooling fixture as a mold for the epoxy, and the potted relay  
>>> looks
>> like
>>> this:
>>>
>>> http://stevezeva.homestead.com/Potted_Relay.jpg
>>>
>>> Has anybody ever heard of this Simonds unit damaging relays like  
>>> this?
>> Has
>>> anybody had to add potting to a relay like this? I can understand  
>>> wanting
>>> to keep the leads coming straight out of the bottom of the body  
>>> before
>>> making the bend to match the footprint on the board, but I think  
>>> I can
>> use
>>> a Bivar permanent spacer and slip it over the lead and accomplish  
>>> the
>> same
>>> thing. Something like this:
>>>
>>>
>> https://www.google.com/url? 
>> sa=t&rct=j&q=&esrc=s&source=web&cd=2&ved=0ahUKEwi
>>> qk8zCt5bOAhWJ1IMKHebaCR8QFggxMAE&url=http%3A%2F%2Fwww.bivar.com
>> %2Fportals%2F
>>> 0%2Fproducts% 
>>> 2F616-070.pdf&usg=AFQjCNESVvvX6qOo_-0T94sAYNLP8AJ21Q&cad=rja
>>>
>>> Or even a nylon washer that matches the diameter of the lead pattern
>>> (.200") coming out of the bottom of the relay. Potting this relay is
>> going
>>> to be very time consuming and there's going to be a risk of  
>>> getting the
>>> epoxy on the leads that will ruin the solderability of the part.  
>>> I'm just
>>> trying to understand if it is truly the Simonds prep unit causing  
>>> the
>>> damage, and if this really is, and easier way other than potting  
>>> them to
>>> accomplish the same thing.
>>>
>>> Thanks all!
>>>
>>> Steve Gregory
>>>
>>> --
>>>
>>>
>>> This email and any attachments are only for use by the intended
>>> recipient(s) and may contain legally privileged, confidential,
>> proprietary
>>> or otherwise private information. Any unauthorized use,  
>>> reproduction,
>>> dissemination, distribution or other disclosure of the contents  
>>> of this
>>> e-mail or its attachments is strictly prohibited. If you have  
>>> received
>>> this
>>> email in error, please notify the sender immediately and delete the
>>> original.
>>>
>>
>
> -- 
>
>
> This email and any attachments are only for use by the intended
> recipient(s) and may contain legally privileged, confidential,  
> proprietary
> or otherwise private information. Any unauthorized use, reproduction,
> dissemination, distribution or other disclosure of the contents of  
> this
> e-mail or its attachments is strictly prohibited. If you have  
> received this
> email in error, please notify the sender immediately and delete the
> original.

ATOM RSS1 RSS2