TECHNET Archives

May 2016

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Show All Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Subject:
From:
"Giamis, Andy" <[log in to unmask]>
Reply To:
TechNet E-Mail Forum <[log in to unmask]>, Giamis, Andy
Date:
Fri, 27 May 2016 15:06:26 +0000
Content-Type:
text/plain
Parts/Attachments:
text/plain (45 lines)
Hi Michael,
With electroplated Sn on your hardware, I'd first be concerned about whiskers.
If you are using electroplated Sn on hardware, have you ever had Sn whisker issues?  Is your hardware anywhere near active, leaded parts.

With Sn finish up against Au, I'd be worried about frit corrosion - but if all you have for Sn plating is mechanical fixtures (no electrical function), I don't think this would be an issue.
As a board finish, immersion Sn has its drawbacks, especially with shelf life and solderability.


-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Kuczynski, Michael
Sent: Friday, May 27, 2016 9:44 AM
To: [log in to unmask]
Subject: [TN] ENIG Board Finish with Tin Plated hardware

We've been using ENIG finish for our PCB's and installing tin plated hardware (self clinching, broaching nuts and standoffs)

We use anywhere from 1 or 2 pieces, to maybe a dozen, of this hardware on various assemblies.
These items are used just to hold or mount some items in place (no serious stress on these items).

Our mfg/assy facility in EU is balking at the finish mismatch and suggesting we change the board finish to immersion tin (which we've never used).

We've built all these assemblies, many, many times without issue.

Is there any other merits I should consider, before I tell them please build them as is?


Michael Kuczynski
Mgr. ECADS - Electrical  511 Benedict Ave.
914-524-3118 (Ph)            Tarrytown, NY 10591
914-524-3322 (Fax)           Mail Stop P25-1-C
[log in to unmask]<mailto:[log in to unmask]>



This message and any attachments are solely for the use of intended recipients. The information contained herein may include trade secrets, protected health or personal information, privileged or otherwise confidential information. Unauthorized review, forwarding, printing, copying, distributing, or using such information is strictly prohibited and may be unlawful. If you are not an intended recipient, you are hereby notified that you received this email in error, and that any review, dissemination, distribution or copying of this email and any attachment is strictly prohibited. If you have received this email in error, please contact the sender and delete the message and any attachment from your system. Thank you for your cooperation

______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask] ______________________________________________________________________

______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask] 
______________________________________________________________________

ATOM RSS1 RSS2