TECHNET Archives

May 2016

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
TechNet E-Mail Forum <[log in to unmask]>, "Kuczynski, Michael" <[log in to unmask]>
Date:
Fri, 27 May 2016 11:47:06 -0400
Reply-To:
TechNet E-Mail Forum <[log in to unmask]>, Yuan-chia Joyce Koo <[log in to unmask]>
Message-ID:
Subject:
From:
Yuan-chia Joyce Koo <[log in to unmask]>
Content-Transfer-Encoding:
7bit
In-Reply-To:
Content-Type:
text/plain; charset="US-ASCII"; delsp=yes; format=flowed
MIME-Version:
1.0 (Apple Message framework v753.1)
Parts/Attachments:
text/plain (67 lines)
> "We've built all these assemblies, many, many times without issue."
you means Siemens didn't have the dissimilar metal coupling check?   
Build is not an issue, corrosion in the field and resistance change  
might be...  it is reliability issue.  if your stuff only work on one  
shot deal (like bomb), and you just engage the two parts upon short  
usage life, not much of issue, if you are in the field for long time  
- like more than 3 month, you should consider dissimilar metal  
coupling from the start of design phase - use some good material/ 
process engineer to select mating parts properly (according to  
standards).
better not be one of those electrical switches... not smart one  
either...
       jk
On May 27, 2016, at 10:43 AM, Kuczynski, Michael wrote:

> We've been using ENIG finish for our PCB's and installing tin  
> plated hardware (self clinching, broaching nuts and standoffs)
>
> We use anywhere from 1 or 2 pieces, to maybe a dozen, of this  
> hardware on various assemblies.
> These items are used just to hold or mount some items in place (no  
> serious stress on these items).
>
> Our mfg/assy facility in EU is balking at the finish mismatch and  
> suggesting we change the board finish to immersion tin (which we've  
> never used).
>
> We've built all these assemblies, many, many times without issue.
>
> Is there any other merits I should consider, before I tell them  
> please build them as is?
>
>
> Michael Kuczynski
> Mgr. ECADS - Electrical  511 Benedict Ave.
> 914-524-3118 (Ph)            Tarrytown, NY 10591
> 914-524-3322 (Fax)           Mail Stop P25-1-C
> [log in to unmask]<mailto:[log in to unmask]>
>
>
>
> This message and any attachments are solely for the use of intended  
> recipients. The information contained herein may include trade  
> secrets, protected health or personal information, privileged or  
> otherwise confidential information. Unauthorized review,  
> forwarding, printing, copying, distributing, or using such  
> information is strictly prohibited and may be unlawful. If you are  
> not an intended recipient, you are hereby notified that you  
> received this email in error, and that any review, dissemination,  
> distribution or copying of this email and any attachment is  
> strictly prohibited. If you have received this email in error,  
> please contact the sender and delete the message and any attachment  
> from your system. Thank you for your cooperation
>
> ______________________________________________________________________
> This email has been scanned by the Symantec Email Security.cloud  
> service.
> For more information please contact helpdesk at x2960 or  
> [log in to unmask]
> ______________________________________________________________________


______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask] 
______________________________________________________________________

ATOM RSS1 RSS2