Do you have cross section photo?
On Tue, Apr 5, 2016 at 10:29 AM, Zilber Gil <[log in to unmask]> wrote:
> Hi All,
> I have an attenuator (ceramic body) with the following pad layers:
> 1. Pd - adhesion layer
> 2. Au- 4 micrometer
> 3. Ni - 1.8 micrometer
> 4. SnPb
>
> This is the first time I am seeing such a pad construction. Does anyone
> have an idea if I should expect any reliability issue (aerospace
> application)?
>
>
> Thanks,
>
>
> Dr. Gil Zilber
> Elta Systmes Ltd.
>
>
>
> The information contained in this communication is proprietary to Israel
> Aerospace Industries Ltd. and/or third parties, may contain confidential or
> privileged information, and is intended only for the use of the intended
> addressee thereof. If you are not the intended addressee, please be aware
> that any use, disclosure, distribution and/or copying of this communication
> is strictly prohibited. If you receive this communication in error, please
> notify the sender immediately and delete it from your computer.
>
>
> ______________________________________________________________________
> This email has been scanned by the Symantec Email Security.cloud service.
> For more information please contact helpdesk at x2960 or [log in to unmask]
> ______________________________________________________________________
>
______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask]
______________________________________________________________________
--
Best Regards,
*Reuven Rokah*
Mobile: 972-52-6012018
Tel: 972-3-9360688
Fax: 15339360688
<http://www.rokah-technologies.com/>[log in to unmask]
[log in to unmask]
www.rokah-technologies.com
The exclusive Israeli agent of:
http://www.greensofttech.com/
This e-mail message is intended for the recipient only and contains
information which is CONFIDENTIAL and which may be proprietary of Rokah
Technologies. If you have received this transmission in error, please
inform me by e-mail, phone or fax, and then please delete all of the
original files and all other copies exist.
______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask]
______________________________________________________________________
|
|
|