Ioan,
With only a 4 hour pot life, you won't have much screen life at all.
As the adhesive gets wiped across the stencil, and large surfaces of the
adhesive get exposed to the air, its properties will change quickly.
For example, I used to use a single part Ablestik material that had a 7 day
pot life!! We only allowed its use on a stencil/screen printing application
for 8 hrs before we discarded it. You could detect the rheological changes,
even then.
If you need to attain and maintain that kind of print geometry, I recommend
you search for another adhesive with a much longer pot life...
Alternatively, they do make some really small dispense needles, but with the
short pot life I still think you have a challenge in front of you
Steve C
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Ioan Tempea
Sent: Friday, April 29, 2016 9:29 AM
To: [log in to unmask]
Subject: [TN] Stencil printing of conductive epoxy
Dear Technos,
I need to stencil print 4 mil in diameter, as thick as possible, dots of the
Epotek E4110-PFC, see
http://www.epotek.com/site/administrator/components/com_products/assets/file
s/Style_Uploads/E4110.pdf
What is your experience with this material?
Any suggestions regarding stencil design/squeegee material/printing program
parameters?
Thanks,
Ioan Tempea, P. Eng.
Manufacturing Engineer, Satellite Systems
[cid:[log in to unmask]]
MacDonald, Dettwiler and Associates Corporation, 21025 Trans-Canada Highway,
Ste-Anne-de-Bellevue, QC, Canada H9X 3R2
Tel: +1-514-457-2150 x3556
www.mdacorporation.com<http://www.mdacorporation.com/>
This e-mail, and any attachments, are intended solely for the use of the
intended recipient(s) and may contain legally privileged, proprietary and/or
confidential information. Any use, disclosure, dissemination, distribution
or copying of this e-mail and any attachments for any purposes that have not
been specifically authorized by the sender is strictly prohibited. If you
are not the intended recipient, please immediately notify the sender by
reply e-mail and permanently delete all copies and attachments. This email
is for informational purposes only and shall not be interpreted to authorize
or conclude a binding agreement between MDA and any other party unless this
email contains or is accompanied by an express written confirmation of MDA's
intention to enter into a binding agreement, such confirmation shall only be
provided by an authorized representative of MDA.
______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask]
______________________________________________________________________
______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask]
______________________________________________________________________
|