Jim,
Temp cycle range is +50°C to +125°C.
I dont have yet the temp ramp rate.
brgds,Ricardo
>>> "Maguire, James F" <[log in to unmask]> 18/04/2016 19:02
>>>
What is temp cycle condition again? You have 50 to 125C but did you
mean -50C to +125C? Also are you doing temp cycle or air/air temp shock
(ie. what is ramp rate in chamber or better yet as measured on the
product during temp cycle).
Jim Maguire
Intel Corporation
ATD Q&R Stress Lab Operations
Hawthorne Farms; Oregon
Engineer
Phone: 503-696-3309
Cell: 253-651-9373
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Ricardo
Moncaglieri
Sent: Monday, April 18, 2016 2:58 PM
To: [log in to unmask]
Subject: Re: [TN] Solder Cracking After Thermal Cicling
Steve,
Responding your question.
Soldered connection is not put under vibration during temp cicling.
This terminal belongs to a connector which is screwed on a case and its
terminal passes through this metalic case and lyies on the pcb ENEPIG
pad.
So that there are following CTEs playing and intercating each other
all
together:
PCB CTE
Solder CTE
Case CTE where is screwed the conector
Terminal CTE
brgds,Ricardo
>>> Steve Gregory <[log in to unmask]> 18/04/2016 18:47 >>>
Hi Ricardo,
I finally have your pictures up, they are here:
http://stevezeva.homestead.com/A15_Photos_of_pre__post_100_temp_cycling_CSC-10_SN12.pdf
Boy, that looks like a big CTE mis-match. A question; are the boards
going through ESS? Vibration along with the temp cycling?
Steve
On Mon, Apr 18, 2016 at 2:35 PM, Ricardo Moncaglieri <
[log in to unmask]> wrote:
> Steve,
> Attached arethe pictures.
> Thank you a lot.
> Await for your comments.
> brgds,Ricardo
>
> >>> Steve Gregory <[log in to unmask]> 18/04/2016 15:22 >>>
> Hi Ricardo,
>
> The Technet server strips the attachments, send your photo directly
to me
> and I'll get it posted...
>
> Steve
>
> On Mon, Apr 18, 2016 at 11:43 AM, Ricardo Moncaglieri <
> [log in to unmask]> wrote:
>
> > Dear colleagues;
> >
> > Steve Gregory, could you please upload the enclosed picture?
> >
> > Solder become perturbated / cracked after thermal cicling:
> >
> > This picture corresponds to a plane (not circular) conector
terminal
> > solded to a pcb pad ENEPIG finished.
> > The connector terminal has been gold removed by twice pretin.
> > Solder used is Sn63Pb37.
> > Thermal cicling: 50°C to 125°C
> >
> > As picture showed there are stretch marks toward left direction
and
> > showed solder crack.
> >
> > Our provider reported temperature didnt pass over 125°C and solder
used
> > 63/37.
> >
> > Question:
> >
> > How could these kind of gooves or stretch marks have been produced
> > taking into account they are just toward one direction (left) and
of
> > considerable length?
> > Just mecanic stress?
> > Temperature overpassing on any cicle?
> > Need of use of different alloy, ie.: In, Bi etc?
> > Provider reported the process is being useed from them since long
ago
> > (same solder alloy, temperature, pcb, terminal conector, thermal
> > cicling) but this is the first time they faced with such a
cracking.
> >
> > Do you have any comment in order to anlyse/solve this trouble.
> >
> > Appreciate your feedback we are in middle of a providing
acceptance
> > tests space quality level (IPC class 3).
> >
> > brgds,Ricardo
> >
> >
> >
> >
______________________________________________________________________
> > This email has been scanned by the Symantec Email Security.cloud
service.
> > For more information please contact helpdesk at x2960 or
> [log in to unmask]
> >
______________________________________________________________________
> >
>
> --
>
>
> This email and any attachments are only for use by the intended
> recipient(s) and may contain legally privileged, confidential,
proprietary
> or otherwise private information. Any unauthorized use,
reproduction,
> dissemination, distribution or other disclosure of the contents of
this
> e-mail or its attachments is strictly prohibited. If you have
received
> this
> email in error, please notify the sender immediately and delete the
> original.
>
>
______________________________________________________________________
> This email has been scanned by the Symantec Email Security.cloud
service.
> For more information please contact helpdesk at x2960 or
[log in to unmask]
>
______________________________________________________________________
>
______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud
service.
For more information please contact helpdesk at x2960 or
[log in to unmask]
______________________________________________________________________
______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask]
______________________________________________________________________
--
This email and any attachments are only for use by the intended
recipient(s) and may contain legally privileged, confidential,
proprietary
or otherwise private information. Any unauthorized use, reproduction,
dissemination, distribution or other disclosure of the contents of
this
e-mail or its attachments is strictly prohibited. If you have received
this
email in error, please notify the sender immediately and delete the
original.
______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud
service.
For more information please contact helpdesk at x2960 or
[log in to unmask]
______________________________________________________________________
______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud
service.
For more information please contact helpdesk at x2960 or
[log in to unmask]
______________________________________________________________________
|