Splash on wavesolder from solder splashing up onto pcb. Can be from poorly adjusted backgate on wavesollder, deep pallets pushing through wave. This is easily removed. Can cause bridging later if it rolls around.
Mike Fenner <[log in to unmask]> wrote:
>OK Maybe there is a difference in language here (British versus US English)
>Irrespective of what IPC says
>I would say in British English that Solder webbing is as already defined:
>traces of solder left adhering to between pads area usually caused by
>inadequate fluxing during wave soldering. If quite bad this can be quite
>large areas. Less severe it used to be described as snails trails. Lesser
>still could be just individual balls.
>These are not the same as splatter which is solder balls ejected from say
>through holes by escaping volatiles, or the same from some solder pastes in
>surface mount or excess solder.
>
>So yes webbing could look the same as spatter. In either case you have
>solder [possibly mobile] on the surface of the board which is not desirable,
>but the cause and therefore cure would be different. Alternatively in the
>case of small balls you could post solder clean the boards to remove them.
>
>--
>Regards
>
>Mike
>
>
>-----Original Message-----
>From: TechNet [mailto:[log in to unmask]] On Behalf Of Ong Seet Leng
>Sent: Tuesday, April 05, 2016 6:27 AM
>To: [log in to unmask]
>Subject: [TN] QUERIES
>
>Afternoon Tech netters,
>
>Apologize for asking the same question again. I may not have put it
>correctly in my email send yesterday. Here it is: how do one tell the
>difference between a solder splatter and solder webbing especially to
>someone who has no knowledge of soldering anomalies. At a first glance, it
>may look the same and cannot differentiate between them.
>
>Please advise.
>
>Regards,
>Seet Leng
>
>______________________________________________________________________
>This email has been scanned by the Symantec Email Security.cloud service.
>For more information please contact helpdesk at x2960 or [log in to unmask]
>______________________________________________________________________
>
>
>______________________________________________________________________
>This email has been scanned by the Symantec Email Security.cloud service.
>For more information please contact helpdesk at x2960 or [log in to unmask]
>______________________________________________________________________
______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask]
______________________________________________________________________
|
|
|