TECHNET Archives

March 2016

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Show All Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Subject:
From:
"lduso - Diamond-MT.com" <[log in to unmask]>
Reply To:
TechNet E-Mail Forum <[log in to unmask]>, lduso - Diamond-MT.com
Date:
Wed, 30 Mar 2016 17:10:01 -0400
Content-Type:
text/plain
Parts/Attachments:
text/plain (154 lines)
For our spray room, we bought one of these
<http://t.sidekickopen48.com/e1t/c/5/f18dQhb0S7lC8dDMPbW2n0x6l2B9nMJN7t5XYgdVhPKW4WYq3x5wvpw0W7fRL1x56dPnsf3Pj9QP02?t=http%3A%2F%2Fwww.amazon.com%2FAlert-Stamping-15FG-25-15-Watt-Fluorescent%2Fdp%2FB002IVTLMW%3Fie%3DUTF8%26psc%3D1%26redirect%3Dtrue%26ref_%3Doh_aui_search_detailpage&si=6019012419387392&pi=1e7540af-9748-4895-82e3-80a5b2fcf369>
to
quickly look at boards while flashing-off on the table. We swapped the bulb
out for a BLB bulb. The sprayer can look at one or two boards before
continuing on and then again after the hundredth one just sweeping down the
table, looking for any major defects like serious dewetting or missed
coverage.

Lloyd Duso
Diamond-MT
Plant Manager
(814) 535-3505
www.Diamond-mt.com

On Wed, Mar 30, 2016 at 4:52 PM, lduso - Diamond-MT.com <
[log in to unmask]> wrote:

> The first flashlight we bought came with them and it seemed to work well
> with Conathane and Dow SR. Humiseal glows crazy bright on it's own.
> Actually, they only enhance certain UV pigments (like urine) but they do
> increase contrast in low light, like in our "cave" where we inspect and
> hand-coat, and they have UV blocking safety 'cause sometimes they all like
> to stare into the pretty purple light!! (That might be because of the fumes
> from the 1B73 though)
>
> Lloyd Duso
> Diamond-MT
> Plant Manager
> (814) 535-3505
> www.Diamond-mt.com
>
> On Wed, Mar 30, 2016 at 4:21 PM, Douglas Pauls <
> [log in to unmask]> wrote:
>
>> Interesting.  What would be the yellow filter you are referring to. Did
>> not see it on the product you had listed in the link.
>>
>>
>> Doug Pauls
>> Principal Materials and Process Engineer
>> Rockwell Collins
>>
>> On Wed, Mar 30, 2016 at 3:16 PM, lduso - Diamond-MT.com <
>> [log in to unmask]> wrote:
>>
>>> Hell Steve, you just had to ask! I equip all my QAs with these. usually
>>> buy
>>> them in batches of 10-20 for $2-3 each direct from China. Plus you can
>>> buy
>>> the yellow tinted lenses to really make it pop. (Learned that from CSI
>>> Miami!!)
>>>
>>> UV flashlights
>>> <
>>> http://t.sidekickopen48.com/e1t/c/5/f18dQhb0S7lC8dDMPbW2n0x6l2B9nMJN7t5XYgdVhPKW4WYq3x5wvpw0W7fRL1x56dPnsf3Pj9QP02?t=http%3A%2F%2Fwww.ebay.com%2Fsch%2Fi.html%3F_from%3DR40%26_trksid%3Dp2050601.m570.l1313.TR3.TRC1.A0.H0.Xplasma%2Betch.TRS0%26_nkw%3Duv%2Bflashlights%26ghostText%3D%26_sacat%3D0&si=6019012419387392&pi=732d3180-656d-4196-d302-9c959b9eee40
>>> >
>>>
>>> Or send somebody down to Spencer Gifts in the Mall. I can't go in there
>>> anymore because my shoes and work jeans start glowing. Even around my
>>> finger nails. I get funny looks but I just tell them I have been
>>> performing
>>> alien autopsies near Roswell.
>>>
>>> Lloyd Duso
>>> Diamond-MT
>>> Plant Manager
>>> (814) 535-3505
>>> www.Diamond-mt.com
>>>
>>> On Wed, Mar 30, 2016 at 3:52 PM, Brian Stumm <
>>> [log in to unmask]> wrote:
>>>
>>> > UV LED's are commonly around 385nm (ranging from 365 to 405nm) which
>>> works
>>> > well for fluorescing coatings. You can find high power UV LED
>>> flashlights
>>> > on ebay for less if you are willing to wait on shipping. Try to keep
>>> below
>>> > 390nm wavelength.
>>> >
>>> > On Wed, Mar 30, 2016 at 12:35 PM, Steve Gregory <[log in to unmask]>
>>> > wrote:
>>> >
>>> > > Hi all,
>>> > >
>>> > > Just discovered something neat today. For $9.97 at Walmart, you can
>>> buy a
>>> > > Rayovac UV LED flashlight that's sold as a pet urine detector that
>>> works
>>> > > wonderfully as a conformal coat inspection light! Even in ambient
>>> light
>>> > on
>>> > > the production floor!
>>> > >
>>> > > Who would have thunk?
>>> > >
>>> > > Steve Gregory
>>> > >
>>> > >
>>> > >
>>> ______________________________________________________________________
>>> > > This email has been scanned by the Symantec Email Security.cloud
>>> service.
>>> > > For more information please contact helpdesk at x2960 or
>>> > [log in to unmask]
>>> > >
>>> ______________________________________________________________________
>>> > > --
>>> > >
>>> > >
>>> > > This email and any attachments are only for use by the intended
>>> > > recipient(s) and may contain legally privileged, confidential,
>>> > proprietary
>>> > > or otherwise private information. Any unauthorized use, reproduction,
>>> > > dissemination, distribution or other disclosure of the contents of
>>> this
>>> > > e-mail or its attachments is strictly prohibited. If you have
>>> received
>>> > this
>>> > > email in error, please notify the sender immediately and delete the
>>> > > original.
>>> > >
>>> >
>>> >
>>> >
>>> >
>>> > ______________________________________________________________________
>>> > This email has been scanned by the Symantec Email Security.cloud
>>> service.
>>> > For more information please contact helpdesk at x2960 or
>>> [log in to unmask]
>>> > ______________________________________________________________________
>>> > --
>>> > Brian Stumm
>>> > ETS, Inc.
>>> > +1-509-276-2015
>>> >
>>>
>>> ______________________________________________________________________
>>> This email has been scanned by the Symantec Email Security.cloud service.
>>> For more information please contact helpdesk at x2960 or
>>> [log in to unmask]
>>> ______________________________________________________________________
>>>
>>
>>
>

______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask] 
______________________________________________________________________

ATOM RSS1 RSS2