All three, and yes, at least one application for space use (stellar positioning system). That one was for a client in Europe. It needed to be lead-free for reasons other than environmental impact (not RoHS-related). It has been working flawlessly for 9 years. The selective solder application was medical, and I have never heard of any failures related to that product either. The wire was used extensively over many industrial and commercial applications, with ditto results; no issues reported.
One thing I have noticed about the wire, the operators really like working with it in that it wets out and fills either the SMT pad or the PTH when doing hand soldering. In their words; "It's just like working with Sn63".
I am sure Kester can provide a lot more information on applications where it has been used than I can, and I am sure they would be happy to.
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Ioan Tempea
Sent: Tuesday, March 08, 2016 9:18 AM
To: [log in to unmask]
Subject: Re: [TN] SAC x SN100C
Hi Dean,
When naming the K100LD, are you implying bar, paste and wire or only one in particular?
Have you used it on space flight hardware also?
Thanks,
Ioan Tempea, P. Eng.
Manufacturing Engineer, Satellite Systems
MacDonald, Dettwiler and Associates Corporation, 21025 Trans-Canada Highway, Ste-Anne-de-Bellevue, QC, Canada H9X 3R2
Tel: +1-514-457-2150 x3556
www.mdacorporation.com
This e-mail, and any attachments, are intended solely for the use of the intended recipient(s) and may contain legally privileged, proprietary and/or confidential information. Any use, disclosure, dissemination, distribution or copying of this e-mail and any attachments for any purposes that have not been specifically authorized by the sender is strictly prohibited. If you are not the intended recipient, please immediately notify the sender by reply e-mail and permanently delete all copies and attachments. This email is for informational purposes only and shall not be interpreted to authorize or conclude a binding agreement between MDA and any other party unless this email contains or is accompanied by an express written confirmation of MDA's intention to enter into a binding agreement, such confirmation shall only be provided by an authorized representative of MDA.
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Stadem, Richard D.
Sent: March-08-16 9:30 AM
To: [log in to unmask]
Subject: Re: [TN] SAC x SN100C
Which SN100C? The properties of SN100C from one vendor such as Kester K100LD are completely different than any SAC305, and also different from other Sn100C alloys. It depends on the dopant added. I have used K100LD for many military applications only because I became very familiar with it during testing of its properties at the Navy testing site on a special project. It has both drop shock and load cycling properties that are quite similar to Sn63, and was selected by the Navy as a preferred alloy over the much more brittle Sn100C alloys that are out there.
http://www.kester.com/kester-content/uploads/2013/03/Tin-Copper_Based_Solders-for_Electronic_Assembly.pdf
I have no financial interest or any other association with Kester. I am only suggesting this alloy because it has proven to be a very good alternative if you need a lead-free that has better wetting as well as an improvement in the modulus of elasticity than Sn100C or, God forbid, SAC305. And it is much less costly.
It has been several years since I qualified this alloy, however. There may be many other new products out there. Just be sure you look at the cost and some of the performance characteristics (or lack thereof). You need to perform a good qualification based on the product you intend to use the solder on. As an example, many SACxxx alloys simply will not fill the plated through holes in an .093" thick PWB with any mass, as the SAC alloys do not wet very well. There are many things to consider. These are not "minor differences"; they can cause a huge difference in reliability, rework costs, etc.
dean
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Datacom - Juliano Ribeiro
Sent: Tuesday, March 08, 2016 5:34 AM
To: [log in to unmask]
Subject: [TN] SAC x SN100C
Hi to all,
What are the differences about SAC305/0307 vs SN100C (reliability criteria and process specification)?
I read about SAC0307 and SAC305 and the article shown that SAC0307 is better about Drop Shock but the SAC305 is better about Thermal Cycle. I would like the same comparison about SAC vs SN100C.
Thank you a lot
_____________________________
Juliano Bettim Ribeiro
DATACOM
ENGENHARIA DE PROCESSOS
Rua América Nº 1000 - Eldorado do Sul - RS CEP: 92990-000
+55 (51) 8446-2135
+55 (51) 3933-3000
Ramal: 3484
<mailto:[log in to unmask]> [log in to unmask] <http://www.datacom.ind.br/> www.datacom.ind.br
______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask] ______________________________________________________________________
______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask] ______________________________________________________________________
______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask] ______________________________________________________________________
______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask]
______________________________________________________________________
|