TECHNET Archives

March 2016

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
TechNet E-Mail Forum <[log in to unmask]>
Date:
Tue, 8 Mar 2016 07:14:42 -0600
Reply-To:
TechNet E-Mail Forum <[log in to unmask]>, Bob Wettermann <[log in to unmask]>
Subject:
MIME-Version:
1.0
Message-ID:
Content-Type:
text/plain; charset="UTF-8"
From:
Bob Wettermann <[log in to unmask]>
Parts/Attachments:
text/plain (21 lines)
Morning All:

Has anyone had success in soldering Type K Thermocouples to a PCB. The
assembly call for a SAC305 no clean alloy....

There are 2 THole connections that will need to be hand-soldered as part of
this assembly.

Thanks!


______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask] 
______________________________________________________________________
-- 
Bob Wettermann
BEST Inc
[log in to unmask]
Cell: 847-767-5745

ATOM RSS1 RSS2