Hi Bob - there are not a lot of elegant ways to remove surface finishes
from component leads. There are some chemical stripping processes but most
folks just have the component re-tinned by solder dipping. Do you know the
reason they want to remove the surface finish?
Dave Hillman
Rockwell Collins
On Fri, Mar 25, 2016 at 7:48 AM, Bob Wettermann <[log in to unmask]> wrote:
> All:
>
> Thanks for the auger discussions.
>
> Here's another weird one for all of you hardcore metallurgists.
>
> Client has white gold parts covered with 30 micro inches of gold plating.
>
> White gold is Au-60%, Pt 11%, Cu 14%, Ag 7%, Zn 1.5% and Pd 6.5%.
>
> They would like to remove the flash gold ....ideas?
>
> Thanks
>
>
> ______________________________________________________________________
> This email has been scanned by the Symantec Email Security.cloud service.
> For more information please contact helpdesk at x2960 or [log in to unmask]
> ______________________________________________________________________
> --
> Bob Wettermann
> BEST Inc
>
______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask]
______________________________________________________________________
|
|
|