DESIGNERCOUNCIL Archives

February 2016

DesignerCouncil@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
DesignerCouncil <[log in to unmask]>
X-To:
Date:
Wed, 10 Feb 2016 12:36:24 -0500
Reply-To:
"(Designers Council Forum)" <[log in to unmask]>, [log in to unmask]
Subject:
MIME-Version:
1.0
Message-ID:
Content-Transfer-Encoding:
quoted-printable
Content-Type:
text/plain; charset="UTF-8"
From:
Parts/Attachments:
text/plain (237 lines)
Hi Steve,
 

First, the designer is part of a Team.  Each member of the team has a  
different responsibility for the success of the project.  The designer is  
responsible for combining the requirements of the EE and ME into the circuit  
board and making sure it can be processed by manufacturing.  That's  it.  
 
The EE is responsible for the functionality of the electronic design.   The 
ME is responsible for the mechanical functionality of the design. And the  
manufacturing groups are responsible for making sure their processes meet 
the  specs laid out by the design team.  The company is responsible for the 
end  product.
 
The designer may follow up with the other team members to find  out what 
worked and didn't work with the design.  This will help with their  ability to 
produce better future designs.  However, once the EE & ME  have examined 
and approved the design, the manufacturers  have agreed that they can build it 
per the specs, then the  designer is done with their part.  
 
Changes to the design based on a change to the original requirements from  
any of the other team members for any reason, are the start of a new design  
cycle (or REVISION).  The original designer may be part of that revision  
cycle or it may be assigned to another designer.   
 
I've seen variations on this over the years depending on company policies,  
contract negotiations, and miss-understandings of who does what.  Many  
companies have tried to combine the designer responsibilities with either the 
EE  or the ME or even the manufacturers.  These usually creates confusion, 
time  delays, and friction in the team.
 
 If a company has a defined PROCESS and they follow  it, then everything 
goes much smoother (and costs less). Also,  don't rush the process.  The best 
results come from a good steady pace with  everyone doing their part and 
supporting each other instead of looking to place  blame.  Having quick design 
reviews on a weekly basis with the whole team  really helps stop delays down 
the line.
 
Hope that helps,
Cherie  Litson, IPC-CID+/CMIT
Litson1 Consulting
PCB Design Solutions &  Training
206-619-8844 [log in to unmask]  

 
In a message dated 2/10/2016 8:46:58 A.M. Pacific Standard Time,  
[log in to unmask] writes:

Well, I  think that needs to be qualified up front in the design cycle, so 
the correct  types of components and materials are selected to meet the 
specified  requirements. 

That's not really what I'm driving at in my question  though. What I'm 
looking for relates more to how far do we as designers  ACTIVELY go in tracking 
the status of a board once it's assembled and handed  over to EE's or 
manufacturing. Is it our responsibility to know if the board  is performing as it 
should? Are we directly responsible to find out that  information?

Steve Horvath
SR. PCB Designer - CID/ Team Lead
AME  Test Group
O: +1 630.285.5840  | M: +1 630.788.3429



  Please consider the environment before printing this  e-mail


-----Original Message-----
From: DesignerCouncil  [mailto:[log in to unmask]] On Behalf Of Ioan 
Tempea
Sent: Wednesday,  February 10, 2016 10:06 AM
To: [log in to unmask]
Subject: Re: [DC]  Designer's Responsibility ends.....when?

Hi Steve,

You might not  want to hear this, but, besides function, the design shall 
also ensure long  term reliability. And since the long term reliability goes 
all the way until  the end of the life cycle of the product, the designer 
should be liable a long  time after the design is completed and successfully 
tested for  functionality.

I suggest IPC-D-279 as a good reading.

Best  regards,

Ioan Tempea, P. Eng.
Manufacturing Engineer, Satellite  Systems 

MacDonald, Dettwiler and Associates Corporation, 21025  Trans-Canada 
Highway, Ste-Anne-de-Bellevue, QC, Canada H9X 3R2
Tel:  +1-514-457-2150 x3556
www.mdacorporation.com

This e-mail, and any  attachments, are intended solely for the use of the 
intended recipient(s) and  may contain legally privileged, proprietary and/or 
confidential information.  Any use, disclosure, dissemination, distribution 
or copying of this e-mail and  any attachments for any purposes that have 
not been specifically authorized by  the sender is strictly prohibited. If 
you are not the intended recipient,  please immediately notify the sender by 
reply e-mail and permanently delete  all copies and attachments. This email 
is for informational purposes only and  shall not be interpreted to authorize 
or conclude a binding agreement between  MDA and any other party unless 
this email contains or is accompanied by an  express written confirmation of 
MDA's intention to enter into a binding  agreement, such confirmation shall 
only be provided by an authorized  representative of MDA.

-----Message d'origine-----
De :  DesignerCouncil [mailto:[log in to unmask]] De la part de 
Horvath, Steven  Envoyé : Wednesday, February 10, 2016 10:56 AM À :  
[log in to unmask] Objet : [DC] Designer's Responsibility  ends.....when?

Hello:


Just want to get an opinion on a  certain matter. Where does a designers 
responsibility end? After successful  assembly, after successful functional 
tests by EE's? System test? By  responsibility, I mean tracking wise. Should 
we be chasing after EE's to make  sure everything tested out okay, while were 
busy designing another board? How  far do we chase? How far do they (MGMT) 
expect YOU to chase?

Thank  You,




Steve Horvath
SR. PCB Designer - CID/ Team  Lead
AME Test Group
O: +1 630.285.5840  | M: +1  630.788.3429



---------------------------------------------------------------------

*******************************  IMPORTANT MESSAGE 
****************************** This transmission may contain  information that is privileged, 
confidential and/or exempt from disclosure  under applicable law. If you are not 
the intended recipient, you are hereby  notified that any disclosure, 
copying, distribution, or use of the information  contained herein (including any 
reliance thereon) is STRICTLY PROHIBITED. If  you received this transmission 
in error, please immediately contact the sender  and destroy the material in 
its entirety, whether in electronic or hard copy  format. Thank  you.
****************************************************************************
****

______________________________________________________________________
This  email has been scanned by the Symantec Email Security.cloud service.
For  more information please contact helpdesk at x2960 or [log in to unmask]  
______________________________________________________________________


--------------------------------------------------------------------------

______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask] 
______________________________________________________________________
--
-----
DesignerCouncil  Mail List provided as a free service by IPC using LISTSERV 
16.0.
To  unsubscribe, send a message to [log in to unmask] with following text in 
the  BODY (NOT the subject field): SIGNOFF DesignerCouncil.
To temporarily  stop/(restart) delivery of DesignerCouncil send: SET 
DesignerCouncil  NOMAIL/(MAIL) For additional information, or contact Keach 
Sasamori at  [log in to unmask] or 847-615-7100  ext.2815
----------------------------------------------------------------------------
-----

______________________________________________________________________
This  email has been scanned by the Symantec Email Security.cloud service.
For  more information please contact helpdesk at x2960 or [log in to unmask]  
______________________________________________________________________


----------------------------------------------------------------------------
-----
DesignerCouncil  Mail List provided as a free service by IPC using LISTSERV 
16.0.
To  unsubscribe, send a message to [log in to unmask] with following text in
the  BODY (NOT the subject field): SIGNOFF DesignerCouncil.
To temporarily  stop/(restart) delivery of DesignerCouncil send: SET 
DesignerCouncil  NOMAIL/(MAIL)
For additional information, or contact Keach Sasamori at  [log in to unmask] or 
847-615-7100  ext.2815
----------------------------------------------------------------------------
-----

*******************************  IMPORTANT MESSAGE 
******************************
This transmission may  contain information that is privileged, confidential
and/or exempt from  disclosure under applicable law. If you are not the 
intended
recipient, you  are hereby notified that any disclosure, copying, 
distribution,
or use of  the information contained herein (including any reliance 
thereon)  is
STRICTLY PROHIBITED. If you received this transmission in error,  please
immediately contact the sender and destroy the material in its  entirety, 
whether
in electronic or hard copy format. Thank  you.
****************************************************************************
****

______________________________________________________________________
This  email has been scanned by the Symantec Email Security.cloud service.
For  more information please contact helpdesk at x2960 or [log in to unmask]  
______________________________________________________________________


----------------------------------------------------------------------------
-----
DesignerCouncil  Mail List provided as a free service by IPC using LISTSERV 
16.0.
To  unsubscribe, send a message to [log in to unmask] with following text in
the  BODY (NOT the subject field):_ SIGNOFF DesignerCouncil.
To temporarily  stop/(restart) delivery of DesignerCouncil send: SET 
DesignerCouncil  NOMAIL/(MAIL)
For additional information, or contact Keach Sasamori at  [log in to unmask] or 
847-615-7100  ext.2815
----------------------------------------------------------------------------
-----


_ (mailto:[log in to unmask]) 

---------------------------------------------------------------------------------
DesignerCouncil Mail List provided as a free service by IPC using LISTSERV 16.0.
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF DesignerCouncil.
To temporarily stop/(restart) delivery of DesignerCouncil send: SET DesignerCouncil NOMAIL/(MAIL)
For additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
---------------------------------------------------------------------------------

ATOM RSS1 RSS2