TECHNET Archives

January 2016

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Show All Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Subject:
From:
Vladimir <[log in to unmask]>
Reply To:
TechNet E-Mail Forum <[log in to unmask]>, Vladimir <[log in to unmask]>
Date:
Mon, 25 Jan 2016 14:51:38 -0500
Content-Type:
text/plain
Parts/Attachments:
text/plain (66 lines)
The one we were given isn't an IPC‎, but IEC one.

Regards,

Vladimir

Sent from my BlackBerry 10 smartphone on the Rogers network.
  Original Message  
From: Victor Hernandez
Sent: Monday, January 25, 2016 14:45
To: [log in to unmask]
Reply To: TechNet E-Mail Forum
Subject: Re: [TN] Press Fit Pins guideline

Vlad,

Does IPC or any other Industry Standard/bench mark have specs. on PFP?

Victor,

-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Vladimir
Sent: Monday, January 25, 2016 12:43 PM
To: [log in to unmask]
Subject: Re: [TN] Press Fit Pins guideline

You'd have to section them. We have a special spec from one of our customers‎ outlining all requirements.

Regards

‎Vladimir
SENTEC

Sent from my BlackBerry 10 smartphone on the Rogers network.
Original Message
From: Victor Hernandez
Sent: Monday, January 25, 2016 13:40
To: [log in to unmask]
Reply To: TechNet E-Mail Forum
Subject: [TN] Press Fit Pins guideline

Fellow TechNetters:

What is the current IPC guideline/specification for insertion depth of Press Fit Pins. I aware that the Press Fit Pins configuration might vary a little, just as well as board thickness. What is the acceptance criteria I should look for visually and during x-ray imaging.

Victor,


______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask] ______________________________________________________________________

______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask] ______________________________________________________________________

______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask] 
______________________________________________________________________

______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask] 
______________________________________________________________________

ATOM RSS1 RSS2