Yes. I do the same thing. I have a pullback of 0.025 from the board edge and have never had an issue. And I also pull back the power layer 10X.
John Babcock, CID+
Sr. PCB Designer
Esterline Interface Technologies
Featuring
ADVANCED INPUT, GAMESMAN,
and LRE MEDICAL products
600 W. Wilbur Avenue
Coeur d’Alene, ID 83815-9496
Toll Free: 800-444-5923 Ext 1522
Direct: (208) 635-8522
-----Original Message-----
From: DesignerCouncil [mailto:[log in to unmask]] On Behalf Of Jenkins, Jeffrey A @ CSG - LINKABIT
Sent: Wednesday, January 06, 2016 12:33 PM
To: [log in to unmask]
Subject: [EXTERNAL] Re: [DC] pull back clearance on internal planes
Depends.
Typically I run the ground/return layers out as far as possible, and the vendors seem to handle .020 from the edge without issue.
But internal power/signal layers, I keep at least 10X the depth to the nearest ground away from the edge of the ground plane copper to minimize EMI.
So for a power plane, if the nearest gnd plane is .005" away , I'd pull it back from .050" from the ground plane copper edge which is .020" from the board edge for a total of .070".
Typically I set the routing/power layers to .100" from the edge just to make my life simple.
Best Regards,
-Jeffrey
Jeffrey A. Jenkins
Sr. PCB Staff Designer, CID+/CIT
L-3 Communications, Linkabit Division
Work: 858-552-9832
Email: [log in to unmask]
-----Original Message-----
From: DesignerCouncil [mailto:[log in to unmask]] On Behalf Of Brooks, William
Sent: Wednesday, January 06, 2016 3:02 PM
To: [log in to unmask]
Subject: [DC] pull back clearance on internal planes
What do you recommend for clearance from the edge of an internal plane to the board edge?
William Brooks, CID+
Printed Circuit Designer
2747 Loker Ave West
Carlsbad, CA 92010-6603
760-930-7212
Fax: 760.918.8332
Mobile: 760.216.0170
E-mail: [log in to unmask]
_____________________________________________________________________________
Scanned by IBM Email Security Management Services powered by MessageLabs. For more information please visit https://urldefense.proofpoint.com/v2/url?u=http-3A__www.ers.ibm.com&d=CwIGaQ&c=0hKVUfnuoBozYN8UvxPA-w&r=GqPf4ISXrghfCbUKD9QlDBaW_kXUG96s8WAzVBpS0Ks&m=YqllFb_32G4GVlAoMfqeLUClo6ruiwX2TNox6B5GUNg&s=DLsMFc4GkLOYX7-tvUAiikW63cJxcs948nvJ1mbBHl0&e=
This email is intended only for the use of the party to which it is addressed and may contain information that is privileged, confidential, or protected by law. If you are not the intended recipient you are hereby notified that any dissemination, copying or distribution of the email or its contents is strictly prohibited. If you have received this message in error, please notify us immediately, by replying to the message and deleting it from your computer.
WARNING: Internet communications are not assured to be secure or clear of inaccuracies as information could be intercepted, corrupted, lost, destroyed, arrive late or incomplete, or contain viruses. Therefore, we do not accept responsibility for any errors or omissions that are present in this email, or any attachment, that have arisen as a result of e-mail transmission.
_____________________________________________________________________________
______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask] ______________________________________________________________________
---------------------------------------------------------------------------------
DesignerCouncil Mail List provided as a free service by IPC using LISTSERV 16.0.
To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF DesignerCouncil.
To temporarily stop/(restart) delivery of DesignerCouncil send: SET DesignerCouncil NOMAIL/(MAIL) For additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
---------------------------------------------------------------------------------
______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask] ______________________________________________________________________
---------------------------------------------------------------------------------
DesignerCouncil Mail List provided as a free service by IPC using LISTSERV 16.0.
To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF DesignerCouncil.
To temporarily stop/(restart) delivery of DesignerCouncil send: SET DesignerCouncil NOMAIL/(MAIL) For additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
---------------------------------------------------------------------------------
______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask] ______________________________________________________________________
---------------------------------------------------------------------------------DesignerCouncil Mail List provided as a free service by IPC using LISTSERV 16.0.To unsubscribe, send a message to [log in to unmask] with following text inthe BODY (NOT the subject field): SIGNOFF DesignerCouncil.To temporarily stop/(restart) delivery of DesignerCouncil send: SET DesignerCouncil NOMAIL/(MAIL)For additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815---------------------------------------------------------------------------------
______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask]
______________________________________________________________________
---------------------------------------------------------------------------------
DesignerCouncil Mail List provided as a free service by IPC using LISTSERV 16.0.
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF DesignerCouncil.
To temporarily stop/(restart) delivery of DesignerCouncil send: SET DesignerCouncil NOMAIL/(MAIL)
For additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
---------------------------------------------------------------------------------
|